ASTM F436 | Description | Circular Plain Washers | Hardness | Rockwell C-Scale: 45 HRC | Grades Available | ASTM Type 1 and 3 | Dimensional Standards | ASTM F436 | Sizes Available | Nominal Size: ¼ inch – 1¼ inches | Thickness: ¼ inches | Compatible Bolts | ASTM A325 / A354 / A449 / A490 / A687 | Compatible Nuts | ASTM A194 / A563 | | |
|
|
ASTM F436M | Description | Circular Plain Washers | Hardness | Rockwell C-Scale: 45 HRC | Grades Available | ASTM Type 1 and 3 | Dimensional Standards | ASTM F436M | Sizes Available | | Thickness: 26mm | Compatible Bolts | ASTM A325M / A490M / A563M / F568 (Grade 8.8 or higher) | Compatible Nuts | ASTM A194M / A563M | | |
|
|
ASTM F844 | Description | Circular Plain Washers | Hardness | Nil | Grades Available | Carbon Steel | Dimensional Standards | ANSI B18.22.1 | Sizes Available | Type A | Type B | Nominal Size: ¼" - 3" | Nominal Size: #0 - #6 | Thickness: ¼ inch | Thickness: ¼ inch |
| Compatible Bolts | ASTM A325 / A354 / A449 / A490 / A687 | Compatible Nuts | ASTM A194 / A563 |
|
|
DIN EN ISO 7089 | Description | Circular Plain Washers | Hardness | Vickers Pyramid Hardness: 200 HV / 300 HV | Grades Available | Carbon Steel: 4.8 / 6.8 / 8.8 | Stainless Steel: A1, A2, A3, A4, A5, C1, C3, C4 and F1 | Dimensional Standards | DIN EN ISO 7089 | Sizes Available | | Thickness: 1.6mm – 10mm | Compatible Bolts and Nuts | | | 200 HV | 300 HV | Bolts | Up to Grade 8.8 | Up to Grade 10.9 | Nuts | Up to Class 8 | Up to Class 10 |
| | |
|
|
| |
DIN EN ISO 7090 | Description | Circular Plain Washers (Chamfered Outer Diameter) | Hardness | Vickers Pyramid Hardness: 200 HV / 300 HV | Grades Available | Carbon Steel: 4.8 / 6.8 / 8.8 | Stainless Steel: A1, A2, A3, A4, C1, C3, C4 and F1 | Dimensional Standards | DIN EN ISO 7090 | Sizes Available | | Thickness: 1.6mm – 10mm | Compatible Bolts and Nuts | | | 200 HV | 300 HV | Bolts | Up to Grade 8.8 | Up to Grade 10.9 | Nuts | Up to Class 8 | Up to Class 10 |
|
|
|
| |
| Description | Circular Plain Washers | Hardness | Vickers Pyramid Hardness: 100 HV | Grades Available | Carbon Steel: 4.8 / 6.8 / 8.8 | Dimensional Standards | DIN EN ISO 7091 (DIN 126) | Sizes Available | | Thickness: 1.6mm – 10mm | Compatible Bolts | Up to Grade 6.8 | Compatible Nuts | Up to Class 6 |
|
| |
DIN 125, PART 1 and PART 2 | Description | Circular Plain Washers | Hardness | Vickers Pyramid Hardness: 200 HV / 300 HV | Grades Available | Carbon Steel: 4.8 / 6.8 / 8.8 | Stainless Steel: A1, A2, A3, A4, A5, C1, C3, C4 and F1 | Dimensional Standards | DIN 125, PART 1 / PART 2 | Sizes Available | | Thickness: 1.6mm – 10mm | Compatible Bolts and Nuts | | | 200 HV | 300 HV | Bolts | Up to Grade 8.8 | Up to Grade 10.9 | Nuts | Up to Class 8 | Up to Class 10 |
|
|