Metric Coarse Structural HSFG Bolt Grade-8.8 EN14399-4 Preload

SKU: 236
Details
Details

Metric Coarse High Strength Friction Grip HSFG Grade-8.8 EN14399

 

d1M12M16M20M22M24M27M30M36
c max.         0.80         0.80         0.80         0.80         0.80         0.80         0.80         0.80
c min.         0.40         0.40         0.40         0.40         0.40         0.40         0.40         0.40
h max.       12.70       16.70       20.84       22.84       24.84       27.84       30.84       37.00
h min.       11.30       15.30       19.16       21.16       23.16       26.16       29.16       35.00
k max.         7.95       10.75       13.40       14.90       15.90       17.90       19.75       23.55
k min.         7.05         9.25       11.60       13.10       14.10       16.10       17.65       21.45
s max       22.00       27.00       32.00       36.00       41.00       46.00       50.00       60.00
s min.       21.16       26.16       31.00       35.00       40.00       45.00       49.00       58.80
e min.       23.91       29.56       35.03       39.55       45.20       50.85       55.37       66.44
ds min       11.30       15.30       19.16       21.16       23.16       26.16       29.16       35.00
ds max       12.70       16.70       20.84       22.84       24.84       27.84       30.84       37.00
dw min       20.10       24.90       29.50       33.30       38.00       42.80       46.60       55.90
da max       15.20       19.20       24.40       26.40       28.40       32.40       35.40       42.40
b <1253038465054606678
b 125-200-44525660667284
b> 200--656973798597

 

High Strength Friction Grip HSFG Grade-8.8 EN 14399 Metric Coarse Structural H.S.F.G Bolt class 8.8 EN14399-4 Preload

Additional Info
Additional Info
Weight0.0000
MaterialGrade-8.8
Standard NumberEN143993
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand TermHEXAGONCAP,HIGHSTRENGTHFRICTIONGRIP
Diameter M12,M16,M20,M22,M24,M27,M30,M36
Length35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200