Metric Hardened Flat Washer HSFG Hardened Steel BS EN 14399-9

SKU: 2586
Details
Details

Metric Hardened Flat Washer HSFG Hardened Steel BS EN 14399-9

dM16M20M22M24M27M30M36
d1 min      16.10      20.10      22.30      24.20      27.20      30.20      36.20
d1 max      16.35      20.40      22.60      24.50      27.55      30.55      36.55
d2 min      27.70      34.40      37.40      41.40      46.40      50.10      60.10
d2max      29.00      36.00      39.00      43.00      48.00      52.00      62.00
h min        3.70        3.70        3.70        3.70        4.40        4.40        5.40
h max        4.30        4.30        4.30        4.30        5.60        5.60        6.60


Metric Hardened Flat Washer HSFG Hardened Steel BS EN14399-9

Additional Info
Additional Info
Weight0.0000
MaterialHARDENED STEEL
Standard NumberDIN6916
Second Standard-
DriveNon
HeadNON
American Generic Brand TermHIGHSTRENGTHFRICTIONGRIPWASHER
Diameter M12,M16,M20,M22,M24,M27,M30,M36