Smalley Wavo Single Turn Round Wire Wave Spring Steel
Smalley Wavo Single Turn Round Wire Wave Spring Steel
Wavo Springs are produced from round-section wire to provide higher loads while maintaining the accurate loading found in wave springs. As an alternative to Belleville Springs, the Wavo provides similar loads but with an accurate, predictable spring rate.
| Part Number | Operates in a bore dia. | Clears Shaft dia. | Load (lb) | Work Height | Reference Free Height | No of Waves | Wire dia. | Reference Spring Rate (lb/in) |
| YRW-0050 | 0.500 | 0.408 | 35 | 0.052 | 0.062 | 3 | 0.031 | 3,500 |
| YRW-0062 | 0.625 | 0.517 | 50 | 0.064 | 0.077 | 3 | 0.038 | 3,846 |
| YRW-0075 | 0.750 | 0.628 | 70 | 0.076 | 0.092 | 3 | 0.045 | 4,375 |
| YRW-0087 | 0.875 | 0.740 | 80 | 0.086 | 0.104 | 3 | 0.051 | 4,444 |
| YRW-0100 | 1.000 | 0.855 | 90 | 0.095 | 0.116 | 3 | 0.056 | 4,286 |
| YRW-0112 | 1.125 | 0.967 | 100 | 0.102 | 0.127 | 3 | 0.060 | 4,000 |
| YRW-0125 | 1.250 | 1.081 | 110 | 0.110 | 0.138 | 3 | 0.065 | 3,929 |
| YRW-0137 | 1.375 | 1.223 | 120 | 0.095 | 0.121 | 4 | 0.056 | 4,615 |
| YRW-0150 | 1.500 | 1.339 | 130 | 0.102 | 0.128 | 4 | 0.060 | 5,000 |
| YRW-0162 | 1.625 | 1.444 | 140 | 0.110 | 0.137 | 4 | 0.065 | 5,185 |
| YRW-0175 | 1.750 | 1.564 | 150 | 0.113 | 0.144 | 4 | 0.067 | 4,839 |
| YRW-0187 | 1.875 | 1.682 | 160 | 0.119 | 0.155 | 4 | 0.070 | 4,444 |
| YRW-0200 | 2.000 | 1.803 | 170 | 0.124 | 0.165 | 4 | 0.072 | 4,146 |
| YRW-0212 | 2.125 | 1.906 | 180 | 0.129 | 0.162 | 4 | 0.076 | 5,455 |
| YRW-0225 | 2.250 | 2.023 | 190 | 0.136 | 0.168 | 4 | 0.080 | 5,938 |
| YRW-0237 | 2.375 | 2.141 | 200 | 0.141 | 0.178 | 4 | 0.083 | 5,405 |
| YRW-0250 | 2.500 | 2.261 | 210 | 0.144 | 0.185 | 4 | 0.085 | 5,122 |
| YRW-0262 | 2.625 | 2.374 | 220 | 0.153 | 0.203 | 4 | 0.090 | 4,400 |
| YRW-0275 | 2.750 | 2.497 | 230 | 0.154 | 0.212 | 4 | 0.091 | 3,966 |
| YRW-0287 | 2.875 | 2.618 | 240 | 0.158 | 0.210 | 4 | 0.093 | 4,615 |
| YRW-0300 | 3.000 | 2.767 | 250 | 0.141 | 0.179 | 5 | 0.083 | 6,579 |
| YRW-0312 | 3.125 | 2.878 | 260 | 0.144 | 0.184 | 5 | 0.085 | 6,500 |
| YRW-0325 | 3.250 | 2.992 | 270 | 0.153 | 0.190 | 5 | 0.090 | 7,297 |
| YRW-0337 | 3.375 | 3.115 | 280 | 0.154 | 0.195 | 5 | 0.091 | 6,829 |
| YRW-0350 | 3.500 | 3.236 | 290 | 0.158 | 0.201 | 5 | 0.093 | 6,744 |
| YRW-0362 | 3.625 | 3.356 | 300 | 0.161 | 0.206 | 5 | 0.095 | 6,667 |
| YRW-0375 | 3.750 | 3.475 | 310 | 0.166 | 0.212 | 5 | 0.098 | 6,739 |
| YRW-0387 | 3.875 | 3.595 | 320 | 0.170 | 0.208 | 5 | 0.100 | 8,421 |
| YRW-0400 | 4.000 | 3.718 | 330 | 0.170 | 0.225 | 5 | 0.100 | 6,000 |
| YRW-0412 | 4.125 | 3.827 | 335 | 0.175 | 0.221 | 5 | 0.105 | 7,283 |
| YRW-0425 | 4.250 | 3.948 | 345 | 0.178 | 0.225 | 5 | 0.105 | 7,340 |
| YRW-0437 | 4.375 | 4.063 | 350 | 0.187 | 0.240 | 5 | 0.110 | 6,604 |
| YRW-0450 | 4.500 | 4.185 | 360 | 0.187 | 0.247 | 5 | 0.110 | 6,000 |
| YRW-0462 | 4.625 | 4.310 | 365 | 0.187 | 0.253 | 5 | 0.110 | 5,530 |
| YRW-0475 | 4.750 | 4.431 | 375 | 0.190 | 0.257 | 5 | 0.112 | 5,597 |
| YRW-0487 | 4.875 | 4.555 | 380 | 0.190 | 0.264 | 5 | 0.112 | 5,135 |
| YRW-0500 | 5.000 | 4.672 | 390 | 0.195 | 0.265 | 5 | 0.116 | 5,571 |
| YRW-0512 | 5.125 | 4.772 | 400 | 0.200 | 0.274 | 5 | 0.118 | 5,405 |
| YRW-0525 | 5.250 | 4.893 | 410 | 0.204 | 0.279 | 5 | 0.120 | 5,467 |
| YRW-0537 | 5.375 | 5.037 | 420 | 0.187 | 0.245 | 6 | 0.110 | 7,241 |
| YRW-0550 | 5.500 | 5.162 | 430 | 0.187 | 0.251 | 6 | 0.110 | 6,719 |
| YRW-0562 | 5.625 | 5.283 | 440 | 0.190 | 0.245 | 6 | 0.112 | 8,000 |
| YRW-0575 | 5.750 | 5.406 | 450 | 0.190 | 0.251 | 6 | 0.112 | 7,377 |
| YRW-0587 | 5.875 | 5.524 | 460 | 0.197 | 0.262 | 6 | 0.116 | 7,077 |
| YRW-0600 | 6.000 | 5.644 | 470 | 0.200 | 0.268 | 6 | 0.118 | 6,912 |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |