ThreadHD1L1L2TW1PIP
M35.00004.200017.000012.00000.90009.00002 PIP
M46.00005.500017.000012.00000.90009.00002 PIP
M57.50007.000019.000014.00001.200011.00002 PIP
M68.50008.400022.000016.00001.500014.00002 PIP
M88.50009.500022.000016.00001.300014.00002 PIP
M810.000010.800026.000016.00001.800018.00002 PIP
M1010.500012.500026.000016.00001.900018.00002 PIP
M1213.000014.000028.000018.00002.200019.00002 PIP