ThreadHD1L1L2TW1PIPTYPE
M35.00004.200017.000012.00000.90009.00002 PIPAM
M46.00005.500017.000012.00000.90009.00002 PIPAM
M57.50007.000019.000014.00001.200011.00002 PIPAM
M68.50008.400022.000016.00001.500014.00002 PIPAM
M88.50009.500022.000016.00001.300014.00002 PIPAM
M811.000010.500026.000017.00002.000018.00002 PIPAM
M1010.500012.200026.000016.00002.000018.00002 PIPAM
M1212.500015.200029.000017.00002.200020.00002 PIPAM