Metric Coarse Single End Weld Stud Stainless-Steel DIN525
SKU:
2199
Details
Details
Metric Coarse Single End Weld Stud Stainless-Steel DIN525
ds | l | b |
---|
M6 | 130.0000 | 35.0000 |
M8 | 140.0000 | 40.0000 |
M10 | 150.0000 | 45.0000 |
M12 | 170.0000 | 55.0000 |
M14 | 180.0000 | 60.0000 |
M16 | 190.0000 | 65.0000 |
M18 | 200.0000 | 70.0000 |
M20 | 210.0000 | 75.0000 |
M22 | 220.0000 | 80.0000 |
M24 | 230.0000 | 85.0000 |
M27 | 250.0000 | 90.0000 |
M30 | 270.0000 | 105.0000 |
M33 | 290.0000 | 115.0000 |
M36 | 310.0000 | 125.0000 |
M42 | 350.0000 | 145.0000 |
M48 | 390.0000 | 165.0000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Stainless-Steel |
---|
Standard Number | DIN525 |
---|
Second Standard | - |
---|
Drive | Non |
---|
Head | NON |
---|
American Generic Brand Term | - |
---|
Diameter | M6,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M42,M48 |
---|
Length | 130,140,150,170,180,000,000,000,000,000,000,000,000,000,000,000 |
---|