Metric Coarse Hexagon Weld Nut Standard Collar Steel BS7670T4

SKU: 2209
Details
Details
Metric Coarse Hexagon Weld Nut Standard Collar Steel BS7670T4
dM3M4M5M6M8M10M12
b max1.00001.00001.00001.12001.25001.55001.5500
b min0.60000.60000.60000.68000.75000.95000.9500
J max4.47005.97006.96007.960010.450012.450014.7500
J min4.39505.89506.87007.870010.340012.340014.6400
e min8.15009.830010.950012.020015.380018.740020.9100
h max0.55000.65000.70000.75000.90001.15001.4000
h min0.45000.55000.60000.60000.75001.00001.2000
t max0.25000.35000.40000.40000.50000.65000.8000
t min0.15000.25000.30000.30000.35000.50000.6000
m max3.00003.50004.00005.00006.50008.000010.0000
m min2.75003.20003.70004.70006.14007.64009.6400
s max7.50009.000010.000011.000014.000017.000019.0000
s min7.28008.78009.780010.730013.730016.730018.6700
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBS7670T4
Second Standard-
DriveHexagon
HeadNON
American Generic Brand Term-
Diameter M3,M4,M5,M6,M8,M10,M12
LengthNON