Metric Coarse Hexagon Spit Trap Projection Weld Nut Steel BLS060262

SKU: 2218
Details
Details
Metric Coarse Hexagon Spit Trap Projection Weld Nut Steel BLS060262
dM5M6M8M10M12
A max10.000013.000015.000018.000022.0000
A min9.780012.730014.730017.730021.6700
B max11.500015.000017.300020.700025.4000
B min11.050014.380016.680019.790024.4900
C max4.00005.00006.50008.000010.0000
C min3.70004.70006.14007.64009.6400
D max0.57000.99001.06001.28001.5600
D min0.47000.89000.96001.18001.4600
E max1.53002.18002.33002.75003.3300
E min1.03001.78001.93002.35002.9300
F max1.02001.77001.89002.23002.6900
F min0.82001.37001.49001.83002.2900
G max0.26000.46000.49000.58000.7200
G min0.16000.36000.39000.48000.6200
H max5.50006.50008.500010.500012.5000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBLS060262
Second Standard-
DriveHexagon
HeadNON
American Generic Brand TermSPIT TRAP
Diameter M5,M6,M8,M10,M12