Metric Coarse Sems Screws with Lock Washer Grade-5.8 DIN69004
SKU:
2293
Details
Details
Metric Coarse Sems Screws with Lock Washer Grade-5.8 DIN69004
| d | a max | l2 min | din 6907 h | din 6907 d2 |
|---|
| M2.5 | 0.9000 | 4.0000 | 1.2000 | 5.5000 |
| M3 | 1.0000 | 4.0000 | 1.2000 | 6.0000 |
| M3.5 | 1.2000 | 6.0000 | 1.5000 | 7.0000 |
| M4 | 1.4000 | 6.0000 | 1.5000 | 8.0000 |
| M5 | 1.6000 | 6.0000 | 1.8000 | 9.0000 |
| M6 | 2.0000 | 8.0000 | 2.1000 | 11.0000 |
| M8 | 2.5000 | 10.0000 | 2.4000 | 14.0000 |
| M10 | 3.0000 | 12.0000 | 2.7000 | 18.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Grade-5.8 |
|---|
| Standard Number | DIN69004 |
|---|
| Second Standard | ISO10644 |
|---|
| Drive | Various |
|---|
| Head | Various |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | M2.5,M3,M3.5,M2.5,M3,M3.5,M8,M10 |
|---|
| Length | 12,14,16,18,20,22,24,26,28,30,35,40,45,50 |
|---|
Reviews