d1d2d3esl minl max
1.53.00001.10000.75000.17002.00004.0000
23.50001.53001.00000.20002.50006.0000
2.54.00002.01001.25000.20003.00006.0000
2.54.50001.90001.25000.25003.00008.0000
35.00002.49001.50000.20003.00008.0000
36.00002.27001.50000.30003.000012.0000
46.50003.38002.00000.25003.000010.0000
48.00003.05002.00000.40003.000016.0000
58.00004.38002.50000.25003.000010.0000
510.00003.83002.50000.50003.000016.0000
610.00005.02003.00000.40003.000016.0000
Additional Info
Additional Info
Weight0.0000
MaterialCOPPER
Standard NumberDIN7339
Second Standard-
DriveNon
HeadFlat
American Generic Brand Term-
Diameter 1.50,2.00,2.50,2.50,3.00,3.00,4.00,4.00,5.00,5.00,6.00
Length 2.00,2.50,3.00,3.50,4.00,5.00,6.00,7.00,8.00,9.00,10.00,12.00,14.00,16.00