d nom | d max | d min | H max 100deg | H min100deg | E | H max78deg | H min78deg | E |
---|
1/8” | 0.1270 | 0.1210 | 0.2290 | 0.2040 | 0.0420 | 0.2290 | 0.2100 | 0.0620 |
5/32” | 0.1580 | 0.1520 | 0.2910 | 0.2620 | 0.0550 | 0.2900 | 0.2640 | 0.0780 |
3/16” | 0.1900 | 0.1840 | 0.3590 | 0.3240 | 0.0700 | 0.3430 | 0.3160 | 0.0940 |
1/4” | 0.2520 | 0.2460 | 0.4840 | 0.4390 | 0.0950 | 0.4560 | 0.4260 | 0.1250 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | ALUMINIUM-ALUMINIUM |
---|
Standard Number | IFI123 |
---|
Second Standard | - |
---|
Drive | Non |
---|
Head | COUNTERSUNK |
---|
American Generic Brand Term | FLAT |
---|
Diameter | 1/8”,5/32”,3/16”,1/4” |
---|