Metric Blind Pop Rivet Large Flat Head DIN7337C
Metric Blind Pop Rivet Large Flat Head DIN7337C
| d1 | d2 | d2 | d2 | k | dm | l min | l max |
|---|---|---|---|---|---|---|---|
| 3.2 | 9.5000 | 9.5000 | 9.5000 | 1.3000 | 2.00:2.05 | 6.0000 | 16.0000 |
| 4 | 12.0000 | 12.0000 | 12.0000 | 1.6000 | 2.45:2.65 | 6.0000 | 20.0000 |
| 4.8 | 11.0000 | 14.0000 | 16.0000 | 1.8000 | 2.95:3.30 | 8.0000 | 25.0000 |
| 5 | 11.0000 | 14.0000 | 16.0000 | 1.8000 | 2.95:3.30 | 8.0000 | 30.0000 |
Metric Blind Pop Rivet Large Flat Head DIN 7337C
| Weight | 0.0000 |
|---|---|
| Material | VARIOUS |
| Standard Number | DIN7337C |
| Second Standard | ISO15973,ISO16585 |
| Drive | Non |
| Head | Largeflat |
| American Generic Brand Term | POP |
| Diameter | 3.2,4,4.8,5 |
| Length | VARIOUS |