Inch 150 deg LARGE Flat Countersunk Semi Tubular Rivets Steel ANSI B18.7

 

B Nom0.1460.188
B max0.1460.188
B Min0.1410.182
C Max0.3670.478
C Min0.3510.458
D Max0.0510.067
D Min0.0410.053
J Max0.1050.139
J Min0.0990.133
K0.1410.188

 

Inch 150 deg LARGE Flat Countersunk Semi Tubular Rivets Steel ANSI B18.7

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL