Fir Tree Button Nylon
Fir Tree Button Nylon
| Hole | Panel | D | H1 | H2 |
| 3.5 | 0.8 - 5 | 9.1 | 9.5 | 1.5 |
| 4 | 0.8 - 5.9 | 9.1 | 11 | 1.5 |
| 4 | 3.5 - 5 | 14 | 10 | 2.5 |
| 4.5 | 1.5 - 13.8 | 20 | 15.3 | 1.4 |
| 4.8 | 0.8 - 4.6 | 11.1 | 9.5 | 1.8 |
| 4.8 | 0.8 - 7.9 | 11.1 | 12.2 | 1 |
| 4.8 | 0.8 - 7.9 | 18.6 | 12.2 | 2.4 |
| 4.8 | 0.8 - 13 | 11.1 | 17.3 | 1.8 |
| 4.8 | 0.9 - 7.9 | 11.1 | 13 | 1.8 |
| 5.2 | 1.7 - 10 | 19 | 18 | 1.8 |
| 5.6 | 1.5 - 14 | 13 | 19.7 | 2 |
| 5.6 | 2.8 - 11 | 12.7 | 15.2 | 1.5 |
| 5.6 | 4.5 - 12.5 | 16 | 17.2 | 2.1 |
| 6 | 2 - 8 | 19 | 13 | 2 |
| 6 | 3 - 8 | 16 | 15 | 2 |
| 6 | 2 - 12 | 18.6 | 15.7 | 1 |
| 6 | 3 - 11.5 | 17.6 | 19.6 | 2.1 |
| 6 | 3.7 - 9.8 | 16.2 | 11.1 | 1.7 |
| 6.2 | 0.8 - 9.1 | 15.8 | 16.1 | 1.3 |
| 6.35 | 1 - 33 | 12.7 | 35.6 | 2.54 |
| 6.4 | 0.8 - 7.4 | 11.1 | 11.1 | 1.8 |
| 6.4 | 2.3 - 7.3 | 19 | 15.9 | 0.8 |
| 6.4 | 2.3 - 9 | 17.8 | 15.5 | 2.5 |
| 6.4 | 2.3 - 14.2 | 17.8 | 20.3 | 2.5 |
| 6.4 | 2.3 - 20.3 | 17.8 | 26.9 | 2.5 |
| 6.4 | 10.5 - 28.7 | 17.8 | 32.4 | 2.5 |
| 6.4 | 10.7 - 28.8 | 17.8 | 35.1 | 2.5 |
| 6.4 | 3 - 11.9 | 18 | 19.9 | 2.6 |
| 6.4 | 3.6 - 11.4 | 29.8 | 15.5 | 3 |
| 6.5 | 3.6 - 12.6 | 17.9 | 20.7 | 2.1 |
| 6.5 | 1.2 - 11.5 | 19.2 | 16.6 | 1.7 |
| 6.5 - 7 | 1.3 - 12.7 | 17.8 | 12.3 | 2 |
| 6.5 - 7 | 4 - 21 | 17.8 | 28.3 | 2 |
| 6.5 - 7 | 6 - 17.5 | 20 | 25 | 2 |
| 6.6 | 1.1 - 9 | 19.7 | 12.4 | 1.7 |
| 6.6 - 7 | 4.5 - 22.1 | 21.9 | 28.5 | 1.8 |
| 6.6 - 7.1 | 2.5 - 9.5 | 18 | 15.6 | 2.1 |
| 6.7 | 2 - 12 | 18.6 | 15.4 | 1 |
| 6.7 | 3.9 - 14.9 | 17.8 | 20.8 | 2.2 |
| 6.9 | 1.3 - 8 | 14 | 12.3 | 1.4 |
| 6.9 | 2.1 - 14 | 16.2 | 17.1 | 1.7 |
| 7 | 0.8 - 11.9 | 19.3 | 16.4 | 1.9 |
| 7 | 1.2 - 9.9 | 20.5 | 14.5 | 2.1 |
| 7 | 0.7 - 20 | 30 | 35 | 2 |
| 7 | 5 - 16.9 | 19.7 | 22.9 | 1.9 |
| 7 - 7.2 | 0.8 | 14 | 12 | 1.6 |
| 7 - 7.4 | 0.7 - 20 | 18 | 27.3 | 2 |
| 7 - 7.5 | 1.1 - 11.1 | 21.5 | 15.6 | 2.1 |
| 7 - 8.4 | 3.8 - 9.5 | 19.5 | 13.4 | 1.8 |
| 7.1 | 2.6 - 19.6 | 20 | 25.3 | 18 |
| 7.1 | 1.5 - 25.4 | 19 | 30.5 | 2.5 |
| 7.2 | 3 - 12 | 20 | 17.3 | 3.2 |
| 7.2 | 2.5 - 7 | 24 | 15 | 2.5 |
| 7.2 | 2.5 - 9 | 24 | 17 | 2.5 |
| 7.2 | 3 - 10 | 14 | 16 | 2 |
| 7.2 | 3 - 16 | 16 | 23 | 2 |
| 7.2 - 7.4 | 0.7 - 11 | 18 | 22.1 | 2 |
| 7.5 | 2.7 - 11.2 | 29.9 | 18.9 | 2.4 |
| 7.9 | 1 - 15.2 | 15.5 | 23.2 | 2 |
| 7.9 | 1.8 - 18.2 | 24.6 | 24.1 | 1.6 |
| 8 | 2.1 - 11.4 | 14.2 | 16 | 1.4 |
| 8 | 3.1 - 7.7 | 25.2 | 12 | 2.3 |
| 8 | 3.2 - 7.5 | 21 | 13.4 | 2 |
| 8.2 | 1 - 15 | 18.4 | 20.5 | 2.1 |
| 8.2 | 0.7 - 5 | 13 | 12.2 | 1.5 |
| 8.2 - 8.7 | 3 - 15.5 | 17.6 | 20.1 | 2.1 |
| 8.4 | 1.1 - 10 | 17.2 | 17.6 | 1.5 |
| 8.5 | 2.6 - 14.2 | 19.1 | 19 | 1.9 |
| 8.5 | 3.9 - 9.8 | 19.7 | 13 | 2.3 |
| 8.7 | 3.3 - 22.7 | 22.2 | 29.3 | 2.4 |
| 8.8 | 5.5 - 19 | 25 | 23.9 | 1.7 |
| 9.5 | -0 | 35.8 | 23.3 | 3.3 |
| 9.7 | 0.5 - 15 | 21.8 | 21.2 | 2.6 |
| 9.8 | 1 - 15.3 | 18.3 | 21.2 | 2.3 |
| 10 | 1.1 - 10 | 35.9 | 20.7 | 3.1 |
| 10.2 | 7 - 16 | 30 | 20 | 2.5 |
| 10.3 | 2.9 - 14.4 | 25.4 | 20.8 | 2.5 |
Fir Tree Button Nylon black white plastic fur christmas pine
| Weight | 0.0100 |
|---|---|
| Material | Nylon 66 |
| Standard Number | No |
| Second Standard | No |
| Drive | Dome |
| Head | BUTTON |
| American Generic Brand Term | No |
| Diameter | range |
| Length | No |