Metric Countersunk Solid Rivet Big Diameters Steel DIN302
| d1 | d2 | d min | k | e |
|---|---|---|---|---|
| 10 | 14.5000 | 9.4000 | 3.0000 | 5.0000 |
| 12 | 18.0000 | 11.3000 | 4.0000 | 6.0000 |
| 14 | 21.5000 | 13.2000 | 5.0000 | 7.0000 |
| 16 | 26.0000 | 15.2000 | 6.5000 | 8.0000 |
| 18 | 30.0000 | 17.1000 | 8.0000 | 9.0000 |
| 19 | 30.5000 | 18.1000 | 9.0000 | 9.0000 |
| 20 | 31.5000 | 19.1000 | 10.0000 | 10.0000 |
| 22 | 34.5000 | 20.9000 | 11.0000 | 11.0000 |
| 24 | 38.0000 | 22.9000 | 12.0000 | 12.0000 |
| 27 | 42.0000 | 25.8000 | 13.5000 | 13.5000 |
| 30 | 42.5000 | 28.6000 | 15.0000 | 15.0000 |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | DIN302 |
| Second Standard | ISO1051,DIN661 |
| Drive | Non |
| Head | COUNTERSUNK |
| American Generic Brand Term | FLAT |
| Diameter | 10,12,14,16,18,19,20,22,24,27,30 |
| Length | 10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160 |