Huck C6L Lock Bolt

SKU: 2664
Details
Details

Huck C6L Lock Bolt

 

              PDF PRODUCT DETAIL

huck BobTail lock bolt

 

 

 

 

 

 

BRAZIER HEAD STEEL 

Dia NomGrip MinGrip MaxD MaxE MaxF NomPART NoPART No
4.81.64.839.110.61.6C6LBR6-2
4.83.26.440.712.23.2C6LBR6-3
4.84.87.942.313.74.8C6LBR6-4
4.86.49.543.915.36.4C6LBR6-5
4.87.911.145.416.97.9C6LBR6-6
4.89.512.747.018.59.5C6LBR6-7
4.811.114.348.620.111.1C6LBR6-8
4.812.715.950.221.712.7C6LBR6-9
4.814.317.551.823.314.3C6LBR6-10
4.815.919.153.424.915.9C6LBR6-11
4.817.520.655.026.417.5C6LBR6-12
4.819.122.256.628.019.1C6LBR6-13
4.820.623.858.129.620.6C6LBR6-14
4.822.225.459.731.222.2C6LBR6-15
4.823.827.061.332.823.8C6LBR6-16
4.825.428.662.934.425.4C6LBR6-17
4.827.030.264.536.027.0C6LBR6-18
4.828.631.866.137.628.6C6LBR6-19
4.830.233.367.739.130.2C6LBR6-20
4.831.834.969.340.731.8C6LBR6-21
4.833.336.570.842.333.3C6LBR6-22
4.834.938.172.443.934.9C6LBR6-23
4.836.539.774.045.536.5C6LBR6-24
4.838.141.375.647.138.1C6LBR6-25
4.839.742.977.248.739.7C6LBR6-26
4.841.344.578.850.341.3C6LBR6-27
4.842.946.080.451.842.9C6LBR6-28
4.844.547.682.053.444.5C6LBR6-29
4.846.049.283.555.046.0C6LBR6-30
4.847.650.885.156.647.6C6LBR6-31
4.849.252.486.758.249.2C6LBR6-32
6.41.64.842.012.91.6C6LBR8-2
6.43.26.443.614.53.2C6LBR8-3
6.44.87.945.216.14.8C6LBR8-4
6.46.49.546.817.66.4C6LBR8-5
6.47.911.148.419.27.9C6LBR8-6
6.49.512.750.020.89.5C6LBR8-7
6.411.114.351.622.411.1C6LBR8-8
6.412.715.953.224.012.7C6LBR8-9
6.414.317.554.725.614.3C6LBR8-10
6.415.919.156.327.215.9C6LBR8-11
6.417.520.657.928.817.5C6LBR8-12
6.419.122.259.530.319.1C6LBR8-13
6.420.623.861.131.920.6C6LBR8-14
6.422.225.462.733.522.2C6LBR8-15
6.423.827.064.335.123.8C6LBR8-16
6.425.428.665.936.725.4C6LBR8-17
6.427.030.267.438.327.0C6LBR8-18
6.428.631.869.039.928.6C6LBR8-19
6.430.233.370.641.530.2C6LBR8-20
6.431.834.972.243.031.8C6LBR8-21
6.433.336.573.844.633.3C6LBR8-22
6.434.938.175.446.234.9C6LBR8-23
6.436.539.777.047.836.5C6LBR8-24
6.438.141.378.649.438.1C6LBR8-25
6.539.742.980.151.039.7C6LBR8-26
6.441.344.581.752.641.3C6LBR8-27
6.442.946.083.354.242.9C6LBR8-28
6.444.547.684.955.744.5C6LBR8-29
6.446.049.286.557.346.0C6LBR8-30
6.447.650.888.158.947.6C6LBR8-31
6.449.252.489.760.549.2C6LBR8-32
7.93.29.551.719.73.2C6LBR10-4
7.96.412.755.122.96.4C6LBR10-6
7.99.515.958.326.19.5C6LBR10-8
7.912.719.161.529.212.7C6LBR10-10
7.915.922.264.632.415.9C6LBR10-12
7.919.125.467.835.619.1C6LBR10-14
7.922.228.671.038.822.2C6LBR10-16
7.925.431.874.241.925.4C6LBR10-18
7.928.634.977.345.128.6C6LBR10-20
7.931.838.180.548.331.8C6LBR10-22
7.934.941.383.751.534.9C6LBR10-24
7.938.144.586.954.638.1C6LBR10-26
7.941.347.690.057.841.3C6LBR10-28
7.944.550.893.261.044.5C6LBR10-30
7.947.654.096.464.247.6C6LBR10-32
9.53.29.557.321.73.2C6LBR12-4
9.56.412.760.524.86.4C6LBR12-6
9.59.515.963.728.09.5C6LBR12-8
9.512.719.166.831.212.7C6LBR12-10
9.515.922.270.034.415.9C6LBR12-12
9.519.125.473.237.519.1C6LBR12-14
9.522.228.676.440.722.2C6LBR12-16
9.525.431.879.543.925.4C6LBR12-18
9.528.634.982.747.128.6C6LBR12-20
9.531.838.185.950.231.8C6LBR12-22
9.534.941.389.153.434.9C6LBR12-24
9.538.144.592.256.638.1C6LBR12-26
9.541.347.695.459.841.3C6LBR12-28
9.544.550.898.662.944.5C6LBR12-30
9.547.654.0101.866.147.6C6LBR12-32

 

The above table gives an indication of the dimensions and an example of the range; for complete information including collar types and conditions please go to the above product brochure.  

 

 

 

C6L®

The Original Huck Design

5.8 grade small diameter LockBolt 
Made to British Standard B7805: Part 1: 1997: A mark of quality, safety and performance 
Wide flange collar available: Enables installation into non metallic materials 
Pin head style: Brazier, truss, countersunk, specific headstyle for palisade fencing 
Collar style: Standard, flanged, wide flanged and low profile 
Materials: Steel, stainless steel, aluminium 

 

 

huck lock bolt lockbolt c6l c6 huck alcoa arconic

Additional Info
Additional Info
Weight0.0100
Material0
Standard NumberNo
Second StandardNo
Drive0
Head0
American Generic Brand TermNo
Diameter0
LengthNo
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.