Inch Countersunk Semi Tubular Rivets Steel BS3575

 

d max d min L  D nom  D max D min K max K min B nom T nom C
  0.1250.1203/16"7/32"0.2180.2080.0300.0250.0825/32"3/32"
0.1440.1403/16"19/64"0.3000.2900.0350.0300.0995/32"3/32"
0.1560.1513/16"5/16"0.3170.3070.0400.0350.1063/16"1/8"
0.1760.1711/4"5/16"0.3170.3070.0400.0350.1283/16"1/8"
0.1880.1831/4"3/8"0.3640.3540.0450.0400.1367/32"1/8"
0.2150.2105/16"27/64"0.4300.4200.0600.0500.1547/32"1/8"
0.2500.2453/8"15/32"0.4780.4680.0600.0500.1807/32"5/32"
0.3120.3077/16"9/16"0.5620.5470.0700.0600.2341/4"3/16"
0.3750.3701/2"5/8"0.6250.6100.0800.0700.2819/32"7/32"

 