Huck Magna-Lok Blind Fastener

SKU: 2667
Details
Details

Huck Magna-Lok Blind Fastener

 

     PDF PRODUCT DETAIL

huck BobTail lock bolt

 

 

 

 

 

 

Example Protruding head Aluminium

Dia NomGrip MinGrip MaxDrill MinDrill MaxB MaxC MaxD MaxPART NoPART No
4.761.576.864.855.119.782.1618.29MGLPB6-4
4.765.4411.104.855.119.782.1622.35MGLPB6-7
4.7614.2719.024.855.119.782.1630.33MGLPB6-12
4.761.5711.104.855.119.782.1625.91MGLPB6-E
6.352.036.356.636.9113.443.0218.29MGLPB8-4
6.352.039.536.636.9113.443.0224.64MGLPB8-6
6.358.8915.886.636.9113.443.0230.99MGLPB8-10
6.3514.7322.236.636.9113.443.0237.34MGLPB8-14
6.3521.0828.586.636.9113.443.0243.69MGLPB8-18
6.3527.4334.936.636.9113.443.0250.04MGLPB8-22
6.352.0315.886.636.9113.443.0235.69MGLPB8-E
9.533.0514.229.9610.3620.144.4741.91MGLPB12-12
9.5315.8828.589.9610.3620.144.4756.26MGLPB12-18
9.5325.4038.109.9610.3620.144.4765.79MGLPB12-24

 

The above table gives an indication of the dimensions and an example of the range; for complete information and conditions please go to the above product brochure. 


 

 

Magna-Lok®

Wide grip range: Accommodates large variations in joint thickness 
Structural fastener: High shear & tensile strength 
Excellent gap closure capability 
Outstanding hole filling on the blind side: Excellent joint tightness and very resistant to water ingress 
Flush pinbreak: No catching on clothes, skin or goods. Quick and easy visual inspection 
Internal pin locking mechanism: Secure within the rivet body and protected from corrosion 
Headstyles: Protruding, truss, countersunk 
Materials: Steel, Stainless Steel, Aluminium

 

 

 

 

 

 

 

Huck Magna-Lok Blind Fastener magna lok lock magnalok magnalock huck alcoa arconic

Additional Info
Additional Info
Weight0.0100
Material0
Standard NumberNo
Second StandardNo
Drive0
Head0
American Generic Brand TermNo
Diameter0
LengthNo
Reviews