Blind Rivet Nut Standard Aluminium

SKU: 2531
Details
Details

Blind Rivet Nut Standard Aluminium

 

 Holedlgrip mingrip maxb
M46.1611.000.253.009.00
M46.1613.002.504.509.00
M57.1711.500.253.0010.00
M57.1713.502.505.0010.00
M69.1915.500.253.5012.00
M69.1918.003.005.5012.00
M811.11117.000.253.5014.00
M811.11120.003.006.0014.00
M1012.11217.500.253.5015.00
M1012.11220.503.006.0015.00
       
 tightening torque Thread breaking force shear strength 
 Nmlb-ftNkpNkp
M432.208,000815.001,500.00153.00
M585.9011,5001,172.002,200.00224.00
M6128.9021,5002,191.003,900.00397.00
M83022.1028,0002,853.005,100.00520.00
M103828.0030,0003,057.006,000.00611.00

Blind Rivet Nut Standard Aluminium riv rivnut