Dia NomGrip MinGrip MaxDrill MinDrill MaxB MaxC MaxD MaxPART NoPART No
4.82.22.84.95.19.92.615.0MBPR6-M2
4.82.23.84.95.19.92.617.1MBPR6-M3
4.83.24.84.95.19.92.617.7MBPR6-M4
4.84.25.84.95.19.92.618.6MBPR6-M5
4.85.26.84.95.19.92.619.7MBPR6-M6
4.86.27.84.95.19.92.620.7MBPR6-M7
4.87.28.84.95.19.92.621.7MBPR6-M8
4.88.29.84.95.19.92.622.7MBPR6-M9
4.89.210.84.95.19.92.623.7MBPR6-M10
4.810.211.84.95.19.92.624.7MBPR6-M11
4.811.212.84.95.19.92.625.7MBPR6-M12
4.812.213.84.95.19.92.626.7MBPR6-M13
4.813.214.84.95.19.92.627.7MBPR6-M14
6.41.53.56.66.913.43.219.3MBPR8-M2
6.42.84.86.66.913.43.221.9MBPR8-M3
6.43.85.86.66.913.43.223.9MBPR8-M4
6.44.86.86.66.913.43.223.2MBPR8-M5
6.45.87.86.66.913.43.223.9MBPR8-M6
6.46.88.86.66.913.43.224.9MBPR8-M7
6.47.89.86.66.913.43.225.9MBPR8-M8
6.48.810.86.66.913.43.226.9MBPR8-M9
6.49.811.86.66.913.43.227.9MBPR8-M10
6.410.812.86.66.913.43.228.9MBPR8-M11
6.411.813.86.66.913.43.230.0MBPR8-M12
6.412.814.86.66.913.43.230.9MBPR8-M13
6.418.820.86.66.913.43.237.1MBPR8-M19
6.431.833.86.66.913.43.250.3MBPR8-M32
7.93.86.48.38.616.83.928.1MBPR10-3
7.95.17.68.38.616.83.929.3MBPR10-4
7.96.48.98.38.616.83.930.6MBPR10-5
7.97.610.28.38.616.83.931.9MBPR10-6
7.98.911.48.38.616.83.933.2MBPR10-7
7.910.212.78.38.616.83.934.4MBPR10-8
7.911.414.08.38.616.83.935.7MBPR10-9
7.912.715.28.38.616.83.937.0MBPR10-10
4.81.92.84.95.19.92.69.4MBCPR6-M2
4.82.23.84.95.19.92.611.4MBCPR6-M3
4.83.24.84.95.19.92.612.0MBCPR6-M4
4.84.25.84.95.19.92.613.0MBCPR6-M5
4.85.26.84.95.19.92.614.1MBCPR6-M6
4.86.27.84.95.19.92.615.0MBCPR6-M7
4.87.28.84.95.19.92.616.1MBCPR6-M8
4.88.29.84.95.19.92.617.0MBCPR6-M9
4.89.210.84.95.19.92.618.0MBCPR6-M10
6.41.53.56.66.913.43.213.1MBCPR8-M2
6.42.84.86.66.913.43.215.7MBCPR8-M3
6.43.85.86.66.913.43.217.7MBCPR8-M4
6.44.86.86.66.913.43.217.0MBCPR8-M5
6.45.87.86.66.913.43.218.0MBCPR8-M6
6.46.88.86.66.913.43.219.0MBCPR8-M7
6.47.89.86.66.913.43.220.0MBCPR8-M8
6.48.8108.06.66.913.43.2210.0MBCPR8-M9
6.410.8128.06.66.913.43.2230.0MBCPR8-M11
6.412.8148.06.66.913.43.2250.0MBCPR8-M13
6.415.8178.06.66.913.43.2280.0MBCPR8-M16
6.418.8208.06.66.913.43.2310.0MBCPR8-M19
6.424.8268.06.66.913.43.2371.0MBCPR8-M25
6.430.8328.06.66.913.43.2430.0MBCPR8-M31

 

 

The above table gives an indication of the dimensions and an example of the range; for complete information and conditions please go to the above product brochure.  

 

 

 

Magna-Bulb®

Extra large blind side footprint: Ideal for lower strength or thin sheet joint materials 
Structural fastener: Very high shear strength and high tensile strength 
Flush pinbreak: No catching on clothes, skin or goods. Quick and easy visual inspection 
Internal pin locking mechanism: Secure within the rivet body and protected from corrosion 
Headstyles: Protruding 
Materials: Steel

 

 

 

Huck Magna-Bulb Blind Fastener magna bulb magnabulb huck alcoa arconic

Additional Info
Additional Info
Weight0.0100
Material0
Standard NumberNo
Second StandardNo
Drive0
Head0
American Generic Brand TermNo
Diameter0
LengthNo
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.