Metric Taper Pin Stainless-Steel-A1 DIN1
| d | c | a |
|---|---|---|
| M1 | 0.1500 | 0.1200 |
| M1.5 | 0.2300 | 0.2000 |
| M2 | 0.3000 | 0.2500 |
| M2.5 | 0.4000 | 0.3000 |
| M3 | 0.4500 | 0.4000 |
| M4 | 0.6000 | 0.5000 |
| M5 | 0.7500 | 0.6300 |
| M6 | 0.9000 | 0.8000 |
| M6.5 | 1.0000 | 0.8000 |
| M7 | 1.1000 | 0.9000 |
| M8 | 1.2000 | 1.0000 |
| M10 | 1.5000 | 1.2000 |
| M12 | 1.8000 | 1.6000 |
| M13 | 1.9000 | 1.7000 |
| M14 | 2.0000 | 1.8000 |
| M16 | 2.5000 | 2.0000 |
| M20 | 3.0000 | 2.5000 |
| Weight | 0.0000 |
|---|---|
| Material | Stainless-Steel-A1 |
| Standard Number | DIN1 |
| Second Standard | ISO2339 |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | - |
| Diameter | 1,1.5,2,2.5,3,4,5,6,8,10,12,14,16,20 |
| Length | 2,3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200 |