Metric Coiled Roll Spring Tension Pin Standard Stainless-Steel DIN7343

SKU: 2019
Details
Details
Metric Coiled Roll Spring Tension Pin Standard Stainless-Steel DIN7343
D d1  d2 a s
11.05000.95000.30000.0800
1.21.25001.15000.40000.1000
1.51.62001.40000.50000.1300
22.13001.90000.70000.1700
2.52.65002.40000.70000.2100
33.15002.90000.90000.2500
3.53.67003.40001.00000.2900
44.20003.90001.10000.3300
55.25004.85001.30000.4200
66.25005.85001.50000.5000
88.30007.80002.00000.6700
1010.35009.75002.50000.8400
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberDIN7343
Second StandardISO8750
DriveNon
HeadNON
American Generic Brand Term SELOK,SPIROL,HEADLAND
Diameter 0.8,1,1.2,1.5,2,2.5,3,3.5,4,5,6,8,10,12,14,16,20
Length4,5,6,8,10,12,14,16,20,24,25,30,35,40,45,50,55,60,65,70,75,80,90,100,120,150,160,180,200