Inch Coiled Roll Spring Tension Pin Heavy Duty Spring-Steel B18.8.2 Coil

SKU: 2043
Details
Details
Inch Coiled Roll Spring Tension Pin Heavy Duty Spring-Steel B18.8.2Coil
ddMax.Min.d2 maxahole maxhole min
1/16"0.06200.07000.06600.05900.02800.06500.0610
5/64"0.07800.08600.08200.07500.03200.08100.0770
3/32"0.09400.10300.09800.09100.03800.09700.0930
7/64"0.10900.11800.11300.10600.03800.11200.1080
1/8"0.12500.13600.13000.12100.04400.12900.1240
5/32"0.15600.16800.16100.15200.04800.16000.1550
3/16"0.18800.20200.19400.18200.05500.19200.1850
7/32"0.21900.23500.22600.21400.06500.22400.2170
1/4"0.25000.26800.25800.24300.06500.25600.2470
5/16"0.31200.33400.32200.30400.08000.31800.3080
3/8"0.37500.40000.38600.36600.09500.38300.3700
7/16"0.43800.46600.45000.42700.09500.44600.4310
1/2"0.50000.53200.51400.48800.11000.51000.4930
5/8"0.62500.65800.64000.61300.12500.63500.6180
3/4"0.75000.78400.76600.73800.15000.76000.7430
Additional Info
Additional Info
Weight0.0000
MaterialSpring-Steel
Standard NumberB18.8.2Coil
Second Standard-
DriveNon
HeadNON
American Generic Brand Term SELOK,SPIROL,HEADLAND
Diameter 1/16",5/64",3/32",7/64",1/8",5/32",3/16",7/32",1/4",5/16",3/8",7/16",1/2",5/8",3/4"
Length3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4."