Metric Head Less Clevis Pin with Out Pin Hole Steel DIN1443A
| d1 max |
|---|
| 3.0000 |
| 4.0000 |
| 5.0000 |
| 6.0000 |
| 8.0000 |
| 10.0000 |
| 12.0000 |
| 14.0000 |
| 16.0000 |
| 18.0000 |
| 20.0000 |
| 22.0000 |
| 24.0000 |
| 27.0000 |
| 30.0000 |
| 33.0000 |
| 36.0000 |
| 40.0000 |
| 45.0000 |
| 50.0000 |
| 55.0000 |
| 60.0000 |
| 70.0000 |
| 80.0000 |
| 90.0000 |
| 100.0000 |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | DIN1443A |
| Second Standard | ISO2340 |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | - |
| Diameter | 3,4,5,6,8,10,12,14,16,18,20,22,24,27,30,33,36,40,45,50,55,60,70,80,90,100 |
| Length | 6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50 |