d1dk maxdk mincd2l minl max
1.42.70002.30000.42001.50003.00006.0000
1.63.00002.60000.48001.70003.00008.0000
23.70003.30000.60002.15003.000010.0000
2.54.60004.20000.75002.70003.000012.0000
35.45004.95000.90003.20004.000016.0000
47.25006.75001.20004.25005.000020.0000
59.10008.50001.50005.25006.000025.0000
610.800010.20001.80006.30008.000030.0000
814.400013.60002.40008.300010.000035.0000
1016.000014.90003.000010.350012.000040.0000
1219.000017.70003.600012.350016.000040.0000
1626.000023.70004.800016.400020.000040.0000
2031.500030.70006.000020.500025.000040.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN1477
Second StandardISO8747
DriveNon
HeadCOUNTERSUNK
American Generic Brand TermFLAT
Diameter 1.4,1.6,2,2.5,3,4,5,6,8,10,12,16,20