Metric Mushroom Head Solid Rivet Brass DIN662
| d nom | d max | d min | d2 nom | K |
|---|
| 1.6 | 1.6500 | 1.5500 | 3.2000 | 0.9000 |
| 2 | 2.1000 | 1.9000 | 4.0000 | 1.0000 |
| 2.5 | 2.6000 | 2.4000 | 5.0000 | 1.2000 |
| 3 | 3.1000 | 2.9000 | 6.0000 | 1.5000 |
| 3.5 | 3.6000 | 3.4000 | 7.0000 | 1.8000 |
| 4 | 4.1000 | 3.9000 | 8.0000 | 2.1000 |
| 5 | 5.1500 | 4.8500 | 10.0000 | 2.5000 |
| 6 | 6.1500 | 5.8500 | 12.0000 | 3.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | BRASS |
|---|
| Standard Number | DIN662 |
|---|
| Second Standard | ISO1051 |
|---|
| Drive | Non |
|---|
| Head | Mushroom |
|---|
| American Generic Brand Term | TRUSS |
|---|
| Diameter | 1.6,2,2.5,3,3.5,4,5,6 |
|---|
| Length | 3,4,5,6,7,8,10,12,14,16,18,20 |
|---|