Metric Grooved Pin Full Length Parallel Groove Stainless-Steel-A1 DIN1473

SKU: 2023
Details
Details
Metric Grooved Pin Full Length Parallel Groove Stainless-Steel-A1 DIN1473
d1a?1?2d2l minl max
1.50.20000.12000.60001.60008.000020.0000
20.25000.18000.80002.15008.000030.0000
2.50.30000.25001.00002.650010.000030.0000
30.40000.30001.20003.200010.000040.0000
40.50000.40001.40004.250010.000060.0000
50.63000.50001.70005.250014.000060.0000
60.80000.60002.10006.300014.000080.0000
81.00000.80002.60008.300014.0000100.0000
101.20001.00003.000010.350014.0000100.0000
121.60001.20003.800012.350018.0000100.0000
162.00001.60004.600016.400022.0000100.0000
202.50002.00006.000020.500026.0000100.0000
253.00002.50007.500025.500026.0000100.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A1
Standard NumberDIN1473
Second StandardISO8740
DriveNon
HeadNON
American Generic Brand Term-
Diameter 1.5,2,2.5,3,4,5,6,8,10,12,16,20,25
Length8,10,12,14,16,18,20,25,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100