DetailsMetric D Shackles Bow Type Steel DIN82103 DIN 82103
d3 | a | b | d1 | d2 | h |
---|
M4 | 0.06 | 8 | 4 | 8 | 16 |
M5 | 0.10 | 10 | 5 | 10 | 20 |
M6 | 0.16 | 12 | 6 | 12 | 24 |
M8 | 0.25 | 16 | 8 | 16 | 32 |
M10 | 0.40 | 20 | 10 | 20 | 40 |
M12 | 0.60 | 24 | 12 | 24 | 48 |
M16 | 1.00 | 32 | 16 | 32 | 64 |
M20 | 1.60 | 40 | 20 | 40 | 80 |
M22 | 2.00 | 44 | 22 | 44 | 88 |
M24 | 2.50 | 48 | 24 | 48 | 96 |
M27 | 3.00 | 54 | 27 | 54 | 108 |
M30 | 4.00 | 60 | 30 | 60 | 120 |
M36 | 5.00 | 72 | 36 | 72 | 144 |
M39 | 6.00 | 78 | 39 | 78 | 156 |
M45 | 8.00 | 90 | 45 | 90 | 180 |
M48 | 10.00 | 96 | 48 | 96 | 192 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | STEEL |
---|
Standard Number | DIN82103 |
---|
Second Standard | EN13889 |
---|
Drive | - |
---|
Head | - |
---|