d Nom | d Min | dk Max | dk Min | K | Drive |
2.50 | 2.25 | 5 | 4.70 | 1.40 | 1 |
3.00 | 2.75 | 6 | 5.70 | 1.80 | 1 |
3.50 | 3.20 | 7 | 6.64 | 2.00 | 2 |
4.00 | 3.70 | 8 | 7.64 | 2.35 | 2 |
4.50 | 4.20 | 9 | 8.64 | 2.55 | 2 |
5.00 | 4.70 | 10 | 9.64 | 2.85 | 2 |
6.00 | 5.70 | 12 | 11.57 | 3.35 | 3 |
Metric Coarse Pozi Countersunk Chipboard Screw Steel DIN 7505 A
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | STEEL |
---|
Standard Number | DIN7505A |
---|
Second Standard | - |
---|
Drive | Pozi, Cross Recess |
---|
Head | - |
---|
American Generic Brand Term | PARTICLEBOARD,FLAT |
---|
Diameter | 0 |
---|
Length | 0 |
---|