db1b2dsdot
M2475.0000110.0000 - - -
M3085.0000120.0000 - - -
M3695.0000140.0000 -M1222.0000
M42105.0000150.000034.0000M1222.0000
M48120.0000160.000038.0000M1222.0000
M56140.0000170.000045.0000M1626.0000
M64155.0000190.000050.0000M1626.0000
M72170.0000200.000055.0000M1626.0000
M80185.0000220.000065.0000M2033.0000
M90205.0000240.000070.0000M2033.0000
M100225.0000260.000080.0000M2033.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-3.6
Standard NumberDIN797
Second Standard-
DriveNon
HeadNON
American Generic Brand Term PULL,CONE
Diameter M24,M30,M36,M42,M48,M56,M64,M72,M80,M90,M100
Length50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300