Internal Spirolox Retaining Rings Type XEH Aerospace Metric
Internal Spirolox Retaining Rings Type XEH Aerospace Metric
The EH Series metric retaining rings are Smalley's standard Spiral Retaining Rings produced to Metric Aerospace specifications (MA 4017). They fit grooves specifically designed for 2-turn spiral retaining rings and accommodate light to medium duty applications.
Standard Materials:
Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel
N.B. Military & Aerospace parts may require additional finishes and inspection procedures to conform to standard
| Part Number | Housing Diameter | Ring Outside Diameter | Ring Radial Wall Min | Ring Radial Wall Max | Ring Thickness | Groove Diameter | Groove Width | Groove Yield (1) | Ring Shear (2) |
| EH-6 | 6 | 6.35 | 0.33 | 0.53 | 0.38 | 6.30 | 0.51 | 440 | 1,880 |
| EH-7 | 7 | 7.37 | 0.33 | 0.53 | 0.38 | 7.32 | 0.51 | 550 | 2,190 |
| EH-8 | 8 | 8.51 | 0.51 | 0.71 | 0.38 | 8.43 | 0.51 | 840 | 2,500 |
| EH-9 | 9 | 9.60 | 0.64 | 0.84 | 0.64 | 9.50 | 0.74 | 1,100 | 4,740 |
| EH-10 | 10 | 10.62 | 0.64 | 0.84 | 0.64 | 10.52 | 0.74 | 1,270 | 5,270 |
| EH-11 | 11 | 11.79 | 0.76 | 0.96 | 0.64 | 11.71 | 0.74 | 1,900 | 5,790 |
| EH-12 | 12 | 12.89 | 1.02 | 1.22 | 0.60 | 12.70 | 0.70 | 2,050 | 7,950 |
| EH-13 | 13 | 13.95 | 1.02 | 1.22 | 0.89 | 13.75 | 1.00 | 2,410 | 12,110 |
| EH-14 | 14 | 15.07 | 1.27 | 1.47 | 0.89 | 14.85 | 1.00 | 2,930 | 13,040 |
| EH-15 | 15 | 16.14 | 1.27 | 1.47 | 0.89 | 15.90 | 1.00 | 3,290 | 13,970 |
| EH-16 | 16 | 17.15 | 1.27 | 1.47 | 0.89 | 16.95 | 1.00 | 3,740 | 14,900 |
| EH-17 | 17 | 18.32 | 1.52 | 1.73 | 0.89 | 18.05 | 1.00 | 4,390 | 15,830 |
| EH-18 | 18 | 19.39 | 1.52 | 1.73 | 0.89 | 19.10 | 1.00 | 4,820 | 16,760 |
| EH-19 | 19 | 20.48 | 1.52 | 1.73 | 0.89 | 20.17 | 1.00 | 5,460 | 17,690 |
| EH-20 | 20 | 21.51 | 1.78 | 1.98 | 0.89 | 21.22 | 1.00 | 5,940 | 18,620 |
| EH-21 | 21 | 22.56 | 1.78 | 1.98 | 0.89 | 22.27 | 1.00 | 6,550 | 19,550 |
| EH-22 | 22 | 23.65 | 1.78 | 1.98 | 1.07 | 23.37 | 1.20 | 7,390 | 24,630 |
| EH-23 | 23 | 24.69 | 2.03 | 2.24 | 1.07 | 24.42 | 1.20 | 7,950 | 25,750 |
| EH-24 | 24 | 25.73 | 2.03 | 2.24 | 1.07 | 25.47 | 1.20 | 8,650 | 26,870 |
| EH-25 | 25 | 27.03 | 2.03 | 2.24 | 1.07 | 26.67 | 1.20 | 10,230 | 27,990 |
| EH-26 | 26 | 28.07 | 2.03 | 2.24 | 1.07 | 27.77 | 1.20 | 11,270 | 29,110 |
| EH-27 | 27 | 29.11 | 2.49 | 2.69 | 1.27 | 28.87 | 1.40 | 12,360 | 31,170 |
| EH-28 | 28 | 30.10 | 2.49 | 2.69 | 1.27 | 29.87 | 1.40 | 12,820 | 32,330 |
| EH-29 | 29 | 31.21 | 2.49 | 2.69 | 1.27 | 30.95 | 1.40 | 13,840 | 33,480 |
| EH-30 | 30 | 32.28 | 2.49 | 2.69 | 1.27 | 32.00 | 1.40 | 14,610 | 34,640 |
| EH-31 | 31 | 33.32 | 2.49 | 2.69 | 1.27 | 33.05 | 1.40 | 15,550 | 35,790 |
| EH-32 | 32 | 34.23 | 2.49 | 2.69 | 1.27 | 34.00 | 1.40 | 15,880 | 36,950 |
| EH-34 | 34 | 36.46 | 2.87 | 3.07 | 1.27 | 36.20 | 1.40 | 18,210 | 39,260 |
| EH-35 | 35 | 37.55 | 2.87 | 3.07 | 1.27 | 37.30 | 1.40 | 19,600 | 40,410 |
| EH-36 | 36 | 38.68 | 2.87 | 3.07 | 1.27 | 38.40 | 1.40 | 21,040 | 41,560 |
| EH-37 | 37 | 39.60 | 2.87 | 3.07 | 1.27 | 39.40 | 1.40 | 21,620 | 42,720 |
| EH-38 | 38 | 40.77 | 2.87 | 3.07 | 1.27 | 40.50 | 1.40 | 23,130 | 43,870 |
| EH-40 | 40 | 42.91 | 3.12 | 3.33 | 1.57 | 42.50 | 1.75 | 24,350 | 57,090 |
| EH-42 | 42 | 45.01 | 3.12 | 3.33 | 1.57 | 44.60 | 1.75 | 26,590 | 59,950 |
| EH-45 | 45 | 48.13 | 3.12 | 3.33 | 1.57 | 47.70 | 1.75 | 29,590 | 64,230 |
| EH-46 | 46 | 49.28 | 3.12 | 3.33 | 1.57 | 48.80 | 1.75 | 31,370 | 65,660 |
| EH-47 | 47 | 50.32 | 3.89 | 4.09 | 1.57 | 49.90 | 1.75 | 33,190 | 67,080 |
| EH-48 | 48 | 51.46 | 3.89 | 4.09 | 1.57 | 51.00 | 1.75 | 35,070 | 68,510 |
| EH-50 | 50 | 53.66 | 3.89 | 4.09 | 1.57 | 53.20 | 1.75 | 38,960 | 71,370 |
| EH-52 | 52 | 54.30 | 3.12 | 3.33 | 1.25 | 53.79 | 1.42 | 22,790 | 59,090 |
| EH-53 | 53 | 55.32 | 3.12 | 3.33 | 1.25 | 54.79 | 1.42 | 23,230 | 60,230 |
| EH-55 | 55 | 57.38 | 3.38 | 3.58 | 1.25 | 56.85 | 1.42 | 24,910 | 62,500 |
| EH-56 | 56 | 58.40 | 3.38 | 3.58 | 1.25 | 57.85 | 1.42 | 25,360 | 63,640 |
| EH-58 | 58 | 60.43 | 3.38 | 3.58 | 1.25 | 59.85 | 1.42 | 26,270 | 65,910 |
| EH-59 | 59 | 61.54 | 3.38 | 3.58 | 1.25 | 60.93 | 1.42 | 27,870 | 67,050 |
| EH-60 | 60 | 62.57 | 3.38 | 3.58 | 1.25 | 61.99 | 1.42 | 29,220 | 68,180 |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |