External Spirolox Retaining Rings Type XWSM Heavy Duty Inch

SKU: 2459
Details
Details

External Spirolox Retaining Rings Type XWSM Heavy Duty Inch

 

The WSM Series Spirolox Retaining Ring is designed for the toughest retaining ring jobs. WSM series retaining rings use standard industry groove dimensions and are interchangeable with many stamped retaining rings. This series should be specified for thrust loads that demand deep groove, heavy section capacity.

Standard Parts:

1/4"-15" Diameters

Standard Materials:

Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel


Part Number Shaft Diameter  Inside Diameter  Radial Wall   Thickness  Groove Diameter  Groove Width Groove Yield (1)Ring Shear (2)
XWSM-31*       0.312       0.287       0.025       0.025       0.290       0.0292431,200
XWSM-37*       0.375       0.349       0.030       0.025       0.352       0.0293051,442
XWSM-43       0.437       0.409       0.035       0.025       0.412       0.0293861,680
XWSM-46       0.469       0.439       0.045       0.025       0.443       0.0294301,880
XWSM-50       0.500       0.464       0.050       0.035       0.468       0.0395702,530
XWSM-55       0.551       0.514       0.050       0.035       0.519       0.0396202,790
XWSM-56       0.562       0.525       0.050       0.035       0.530       0.0396402,840
XWSM-59       0.594       0.554       0.050       0.035       0.559       0.0397603,000
XWSM-62       0.625       0.583       0.055       0.035       0.588       0.0398403,160
XWSM-66       0.669       0.623       0.055       0.035       0.629       0.0399503,380
XWSM-68       0.688       0.641       0.065       0.042       0.646       0.0461,0204,180
XWSM-75       0.750       0.698       0.065       0.042       0.704       0.0461,2204,550
XWSM-78       0.781       0.727       0.065       0.042       0.733       0.0461,3304,740
XWSM-81       0.812       0.756       0.065       0.042       0.762       0.0461,4404,930
XWSM-87       0.875       0.814       0.075       0.042       0.821       0.0461,6705,310
XWSM-93       0.938       0.875       0.075       0.042       0.882       0.0461,8605,690
XWSM-98       0.984       0.919       0.085       0.042       0.926       0.0462,0205,970
XWSM-100       1.000       0.932       0.085       0.042       0.940       0.0462,1206,070
XWSM-102       1.023       0.953       0.085       0.042       0.961       0.0462,2406,210
XWSM-106       1.062       0.986       0.103       0.050       0.998       0.0562,4007,010
XWSM-112       1.125       1.047       0.103       0.050       1.059       0.0562,6207,420
XWSM-118       1.188       1.105       0.103       0.050       1.118       0.0562,9407,840
XWSM-125       1.250       1.163       0.103       0.050       1.176       0.0563,2708,250
XWSM-131       1.312       1.218       0.118       0.050       1.232       0.0563,7108,660
XWSM-137       1.375       1.277       0.118       0.050       1.291       0.0564,0809,070
XWSM-143       1.438       1.336       0.118       0.050       1.350       0.0564,4709,490
XWSM-150       1.500       1.385       0.118       0.050       1.406       0.0564,9809,900
XWSM-156       1.562       1.453       0.128       0.062       1.468       0.0685,19012,780
XWSM-162       1.625       1.513       0.128       0.062       1.529       0.0685,51013,290
XWSM-168       1.687       1.573       0.128       0.062       1.589       0.0685,84013,800
XWSM-175       1.750       1.633       0.128       0.062       1.650       0.0686,19014,320
XWSM-177       1.771       1.651       0.128       0.062       1.669       0.0686,38014,490
XWSM-181       1.812       1.690       0.128       0.062       1.708       0.0686,66014,820
XWSM-187       1.875       1.751       0.158       0.062       1.769       0.0687,02015,340
XWSM-196       1.969       1.838       0.158       0.062       1.857       0.0687,79016,110
XWSM-200       2.000       1.867       0.158       0.062       1.886       0.0688,06016,360
XWSM-206       2.062       1.932       0.168       0.078       1.946       0.0868,45021,220
XWSM-212       2.125       1.989       0.168       0.078       2.003       0.0869,16021,870
XWSM-215       2.156       2.018       0.168       0.078       2.032       0.0869,45022,190
XWSM-225       2.250       2.105       0.168       0.078       2.120       0.08610,34023,160
XWSM-231       2.312       2.163       0.168       0.078       2.178       0.08610,95023,800
XWSM-237       2.375       2.223       0.200       0.078       2.239       0.08611,42024,440
XWSM-243       2.437       2.283       0.200       0.078       2.299       0.08611,89025,080
XWSM-250       2.500       2.343       0.200       0.078       2.360       0.08612,37025,730
XWSM-255       2.559       2.402       0.200       0.078       2.419       0.08612,66026,340
XWSM-262       2.625       2.464       0.200       0.078       2.481       0.08613,36027,020
XWSM-268       2.687       2.523       0.200       0.078       2.541       0.08613,87027,660
Additional Info
Additional Info
Weight0.0100
Material0
Standard NumberNo
Second StandardNo
Drive0
Head0
American Generic Brand TermNo
Diameter0
LengthNo
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.