External Spirolox Retaining Rings Type XES Aerospace Metric

SKU: 2457
Details
Details

External Spirolox Retaining Rings Type XES Aerospace Metric

 

The ES Series metric retaining rings are Smalley's standard Spiral Retaining Rings produced to Metric Aerospace specifications. They fit grooves specifically designed for 2-turn spiral retaining rings and accommodate light to medium duty applications.

Standard Parts:

12mm - 280mm diameters

Standard Materials:

Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel


Part NumberShaft Diameter Inside Diameter  Radial Wall Min  Radial Wall Max  Thickness  Groove Diameter  Groove Width Groove Yield (1)Ring Shear (2)
XES-77         6.53         0.51         0.71         0.64         6.58         0.747203,690
XES-88         7.49         0.51         0.71         0.64         7.57         0.748404,210
XES-99         8.41         0.64         0.84         0.64         8.48         0.741,1404,740
XES-1010         9.40         0.64         0.84         0.64         9.50         0.741,2205,270
XES-1111       10.39         0.76         0.96         0.64       10.46         0.741,4505,790
XES-1212       11.18         1.02         1.22         0.60       11.29         0.702,1007,950
XES-1313       12.13         1.14         1.35         0.89       12.24         1.002,41012,100
XES-1414       13.06         1.14         1.35         0.89       13.19         1.002,80013,040
XES-1515       13.98         1.14         1.35         0.89       14.09         1.003,36013,970
XES-1616       14.90         1.27         1.48         0.89       15.02         1.003,82014,900
XES-1717       15.82         1.27         1.48         0.89       16.02         1.004,06015,830
XES-1818       16.80         1.52         1.73         1.07       16.92         1.204,73020,150
XES-1919       17.73         1.52         1.73         1.07       17.87         1.205,27021,270
XES-2020       18.62         1.52         1.73         1.07       18.77         1.206,04022,390
XES-2121       19.57         1.52         1.73         1.07       19.72         1.206,55023,510
XES-2222       20.45         1.78         1.98         1.07       20.62         1.207,39024,630
XES-2323       21.39         1.78         1.98         1.07       21.57         1.208,07025,750
XES-2424       22.35         1.78         1.98         1.07       22.52         1.208,65026,870
XES-2525       23.25         2.03         2.24         1.07       23.42         1.209,62027,990
XES-2626       24.21         2.03         2.24         1.07       24.42         1.2010,00029,110
XES-2727       25.04         2.49         2.69         1.27       25.35         1.4010,91031,170
XES-2828       26.00         2.49         2.69         1.27       26.30         1.4011,59032,330
XES-2929       26.95         2.49         2.69         1.27       27.27         1.4012,29033,480
XES-3030       27.92         2.49         2.69         1.27       28.25         1.4012,86034,640
XES-3131       28.84         2.49         2.69         1.27       29.17         1.4013,89035,790
XES-3232       29.77         2.49         2.69         1.27       30.09         1.4014,96036,950
XES-3434       31.54         2.87         3.07         1.27       31.90         1.4017,39039,260
XES-3535       32.44         2.87         3.07         1.27       32.80         1.4018,75040,410
XES-3636       33.40         2.87         3.07         1.27       33.75         1.4019,81041,560
XES-3737       34.24         2.87         3.07         1.27       34.67         1.4021,08042,720
XES-3838       35.18         2.87         3.07         1.27       35.66         1.4021,65043,870
XES-4040       37.15         3.12         3.33         1.57       37.55         1.7523,96057,090
XES-4242       39.02         3.12         3.33         1.57       39.45         1.7526,18059,990
XES-4545       41.77         3.12         3.33         1.57       42.25         1.7530,24064,230
XES-4646       42.67         3.12         3.33         1.57       43.15         1.7532,04065,660
XES-4747       43.81         3.89         4.09         1.57       44.31         1.7530,90067,080
XES-4848       44.48         3.89         4.09         1.57       45.05         1.7534,60068,510
XES-5050       46.69         3.89         4.09         1.57       47.05         1.7536,04071,370
XES-5252       49.62         3.12         3.33         1.25       50.15         1.4223,55059,090
XES-5353       50.62         3.12         3.33         1.25       51.15         1.4224,00060,230
XES-5454       51.62         3.12         3.33         1.25       52.15         1.4224,46061,370
XES-5555       52.62         3.38         3.58         1.25       53.15         1.4224,91062,500
XES-5656       53.62         3.38         3.58         1.25       54.15         1.4225,37063,640
XES-5858       55.43         3.38         3.58         1.25       56.01         1.4228,25065,910
XES-5959       56.43         3.38         3.58         1.25       57.01         1.4228,73067,050

 

Additional Info
Additional Info
Weight0.0100
Material0
Standard NumberNo
Second StandardNo
Drive0
Head0
American Generic Brand TermNo
Diameter0
LengthNo
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.