External Spirolox Retaining Rings Type XWSM Heavy Duty Inch
External Spirolox Retaining Rings Type XWSM Heavy Duty Inch
The WSM Series Spirolox Retaining Ring is designed for the toughest retaining ring jobs. WSM series retaining rings use standard industry groove dimensions and are interchangeable with many stamped retaining rings. This series should be specified for thrust loads that demand deep groove, heavy section capacity.
Standard Parts:
1/4"-15" Diameters
Standard Materials:
Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel
| Part Number | Shaft Diameter | Inside Diameter | Radial Wall | Thickness | Groove Diameter | Groove Width | Groove Yield (1) | Ring Shear (2) |
| XWSM-31* | 0.312 | 0.287 | 0.025 | 0.025 | 0.290 | 0.029 | 243 | 1,200 |
| XWSM-37* | 0.375 | 0.349 | 0.030 | 0.025 | 0.352 | 0.029 | 305 | 1,442 |
| XWSM-43 | 0.437 | 0.409 | 0.035 | 0.025 | 0.412 | 0.029 | 386 | 1,680 |
| XWSM-46 | 0.469 | 0.439 | 0.045 | 0.025 | 0.443 | 0.029 | 430 | 1,880 |
| XWSM-50 | 0.500 | 0.464 | 0.050 | 0.035 | 0.468 | 0.039 | 570 | 2,530 |
| XWSM-55 | 0.551 | 0.514 | 0.050 | 0.035 | 0.519 | 0.039 | 620 | 2,790 |
| XWSM-56 | 0.562 | 0.525 | 0.050 | 0.035 | 0.530 | 0.039 | 640 | 2,840 |
| XWSM-59 | 0.594 | 0.554 | 0.050 | 0.035 | 0.559 | 0.039 | 760 | 3,000 |
| XWSM-62 | 0.625 | 0.583 | 0.055 | 0.035 | 0.588 | 0.039 | 840 | 3,160 |
| XWSM-66 | 0.669 | 0.623 | 0.055 | 0.035 | 0.629 | 0.039 | 950 | 3,380 |
| XWSM-68 | 0.688 | 0.641 | 0.065 | 0.042 | 0.646 | 0.046 | 1,020 | 4,180 |
| XWSM-75 | 0.750 | 0.698 | 0.065 | 0.042 | 0.704 | 0.046 | 1,220 | 4,550 |
| XWSM-78 | 0.781 | 0.727 | 0.065 | 0.042 | 0.733 | 0.046 | 1,330 | 4,740 |
| XWSM-81 | 0.812 | 0.756 | 0.065 | 0.042 | 0.762 | 0.046 | 1,440 | 4,930 |
| XWSM-87 | 0.875 | 0.814 | 0.075 | 0.042 | 0.821 | 0.046 | 1,670 | 5,310 |
| XWSM-93 | 0.938 | 0.875 | 0.075 | 0.042 | 0.882 | 0.046 | 1,860 | 5,690 |
| XWSM-98 | 0.984 | 0.919 | 0.085 | 0.042 | 0.926 | 0.046 | 2,020 | 5,970 |
| XWSM-100 | 1.000 | 0.932 | 0.085 | 0.042 | 0.940 | 0.046 | 2,120 | 6,070 |
| XWSM-102 | 1.023 | 0.953 | 0.085 | 0.042 | 0.961 | 0.046 | 2,240 | 6,210 |
| XWSM-106 | 1.062 | 0.986 | 0.103 | 0.050 | 0.998 | 0.056 | 2,400 | 7,010 |
| XWSM-112 | 1.125 | 1.047 | 0.103 | 0.050 | 1.059 | 0.056 | 2,620 | 7,420 |
| XWSM-118 | 1.188 | 1.105 | 0.103 | 0.050 | 1.118 | 0.056 | 2,940 | 7,840 |
| XWSM-125 | 1.250 | 1.163 | 0.103 | 0.050 | 1.176 | 0.056 | 3,270 | 8,250 |
| XWSM-131 | 1.312 | 1.218 | 0.118 | 0.050 | 1.232 | 0.056 | 3,710 | 8,660 |
| XWSM-137 | 1.375 | 1.277 | 0.118 | 0.050 | 1.291 | 0.056 | 4,080 | 9,070 |
| XWSM-143 | 1.438 | 1.336 | 0.118 | 0.050 | 1.350 | 0.056 | 4,470 | 9,490 |
| XWSM-150 | 1.500 | 1.385 | 0.118 | 0.050 | 1.406 | 0.056 | 4,980 | 9,900 |
| XWSM-156 | 1.562 | 1.453 | 0.128 | 0.062 | 1.468 | 0.068 | 5,190 | 12,780 |
| XWSM-162 | 1.625 | 1.513 | 0.128 | 0.062 | 1.529 | 0.068 | 5,510 | 13,290 |
| XWSM-168 | 1.687 | 1.573 | 0.128 | 0.062 | 1.589 | 0.068 | 5,840 | 13,800 |
| XWSM-175 | 1.750 | 1.633 | 0.128 | 0.062 | 1.650 | 0.068 | 6,190 | 14,320 |
| XWSM-177 | 1.771 | 1.651 | 0.128 | 0.062 | 1.669 | 0.068 | 6,380 | 14,490 |
| XWSM-181 | 1.812 | 1.690 | 0.128 | 0.062 | 1.708 | 0.068 | 6,660 | 14,820 |
| XWSM-187 | 1.875 | 1.751 | 0.158 | 0.062 | 1.769 | 0.068 | 7,020 | 15,340 |
| XWSM-196 | 1.969 | 1.838 | 0.158 | 0.062 | 1.857 | 0.068 | 7,790 | 16,110 |
| XWSM-200 | 2.000 | 1.867 | 0.158 | 0.062 | 1.886 | 0.068 | 8,060 | 16,360 |
| XWSM-206 | 2.062 | 1.932 | 0.168 | 0.078 | 1.946 | 0.086 | 8,450 | 21,220 |
| XWSM-212 | 2.125 | 1.989 | 0.168 | 0.078 | 2.003 | 0.086 | 9,160 | 21,870 |
| XWSM-215 | 2.156 | 2.018 | 0.168 | 0.078 | 2.032 | 0.086 | 9,450 | 22,190 |
| XWSM-225 | 2.250 | 2.105 | 0.168 | 0.078 | 2.120 | 0.086 | 10,340 | 23,160 |
| XWSM-231 | 2.312 | 2.163 | 0.168 | 0.078 | 2.178 | 0.086 | 10,950 | 23,800 |
| XWSM-237 | 2.375 | 2.223 | 0.200 | 0.078 | 2.239 | 0.086 | 11,420 | 24,440 |
| XWSM-243 | 2.437 | 2.283 | 0.200 | 0.078 | 2.299 | 0.086 | 11,890 | 25,080 |
| XWSM-250 | 2.500 | 2.343 | 0.200 | 0.078 | 2.360 | 0.086 | 12,370 | 25,730 |
| XWSM-255 | 2.559 | 2.402 | 0.200 | 0.078 | 2.419 | 0.086 | 12,660 | 26,340 |
| XWSM-262 | 2.625 | 2.464 | 0.200 | 0.078 | 2.481 | 0.086 | 13,360 | 27,020 |
| XWSM-268 | 2.687 | 2.523 | 0.200 | 0.078 | 2.541 | 0.086 | 13,870 | 27,660 |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |