External Spirolox Retaining Rings Type XDNS DIN Series Metric
External Spirolox Retaining Rings Type XDNS DIN Series Metric
The DNS Series Spirolox Retaining Ring is Smalley's equivalent to the European or "Hard" metric retaining ring series. With their 2-turn offset configuration, these spiral rings will fit into the grooves established by DIN specifications.
Standard Parts:
13mm-400mm Diameters
Standard Materials:
Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel
| Part Number | Shaft Diameter | Inside Diameter | Radial Wall Min | Thickness | Groove Diameter | Groove Width | Groove Yield (1) | Ring Shear (2) |
| XDNS-13 | 13 | 12.27 | 1.4 | 0.99 | 12.4 | 1.1 | 1,901 | 13,474 |
| XDNS-14 | 14 | 13.26 | 1.4 | 0.99 | 13.4 | 1.1 | 2,047 | 14,510 |
| XDNS-15 | 15 | 14.15 | 1.4 | 0.99 | 14.3 | 1.1 | 2,559 | 15,547 |
| XDNS-16 | 16 | 15.04 | 1.65 | 0.99 | 15.2 | 1.1 | 3,119 | 16,583 |
| XDNS-17 | 17 | 16.04 | 1.65 | 0.99 | 16.2 | 1.1 | 3,314 | 17,620 |
| XDNS-18 | 18 | 16.83 | 1.91 | 1.14 | 17 | 1.3 | 4,386 | 18,668 |
| XDNS-19 | 19 | 17.83 | 1.91 | 1.14 | 18 | 1.3 | 4,630 | 19,705 |
| XDNS-20 | 20 | 18.82 | 1.91 | 1.14 | 19 | 1.3 | 4,874 | 20,742 |
| XDNS-21 | 21 | 19.79 | 1.91 | 1.14 | 20 | 1.3 | 5,117 | 21,779 |
| XDNS-22 | 22 | 20.78 | 1.91 | 1.14 | 21 | 1.3 | 5,361 | 22,816 |
| XDNS-23 | 23 | 21.77 | 1.91 | 1.14 | 22 | 1.3 | 5,605 | 23,853 |
| XDNS-24 | 24 | 22.66 | 2.18 | 1.14 | 22.9 | 1.3 | 6,433 | 24,891 |
| XDNS-25 | 25 | 23.65 | 2.18 | 1.14 | 23.9 | 1.3 | 6,701 | 25,928 |
| XDNS-26 | 26 | 24.64 | 2.18 | 1.14 | 24.9 | 1.3 | 6,969 | 26,965 |
| XDNS-27 | 27 | 25.34 | 2.18 | 1.14 | 25.6 | 1.3 | 9,211 | 28,002 |
| XDNS-28 | 28 | 26.34 | 2.39 | 1.44 | 26.6 | 1.6 | 9,552 | 36,681 |
| XDNS-29 | 29 | 27.33 | 2.39 | 1.44 | 27.6 | 1.6 | 9,893 | 37,991 |
| XDNS-30 | 30 | 28.32 | 2.39 | 1.44 | 28.6 | 1.6 | 10,235 | 39,301 |
| XDNS-32 | 32 | 30 | 3.25 | 1.44 | 30.3 | 1.6 | 13,256 | 41,921 |
| XDNS-33 | 33 | 30.99 | 3.25 | 1.44 | 31.3 | 1.6 | 13,670 | 43,231 |
| XDNS-34 | 34 | 31.98 | 3.25 | 1.44 | 32.3 | 1.6 | 14,085 | 44,541 |
| XDNS-35 | 35 | 32.66 | 3.25 | 1.44 | 33 | 1.6 | 17,058 | 45,851 |
| XDNS-36 | 36 | 33.65 | 4.01 | 1.69 | 34 | 1.85 | 17,545 | 55,349 |
| XDNS-38 | 38 | 35.64 | 4.01 | 1.69 | 36 | 1.85 | 18,520 | 58,424 |
| XDNS-40 | 40 | 37.11 | 4.01 | 1.69 | 37.5 | 1.85 | 24,368 | 61,498 |
| XDNS-42 | 42 | 39.09 | 4.01 | 1.69 | 39.5 | 1.85 | 25,586 | 64,573 |
| XDNS-45 | 45 | 42.06 | 4.01 | 1.69 | 42.5 | 1.85 | 27,414 | 69,186 |
| XDNS-46 | 46 | 43.05 | 4.01 | 1.69 | 43.5 | 1.85 | 28,023 | 70,723 |
| XDNS-47 | 47 | 44.04 | 4.01 | 1.69 | 44.5 | 1.85 | 28,633 | 72,261 |
| XDNS-48 | 48 | 45.03 | 4.01 | 1.69 | 45.5 | 1.85 | 29,242 | 73,798 |
| XDNS-50 | 50 | 46.53 | 5.08 | 1.93 | 47 | 2.15 | 36,552 | 87,790 |
| XDNS-52 | 52 | 48.51 | 5.08 | 1.93 | 49 | 2.15 | 38,014 | 91,302 |
| XDNS-54 | 54 | 50.5 | 5.08 | 1.93 | 51 | 2.15 | 39,476 | 94,813 |
| XDNS-55 | 55 | 51.49 | 5.08 | 1.93 | 52 | 2.15 | 40,207 | 96,569 |
| XDNS-56 | 56 | 52.48 | 5.08 | 1.93 | 53 | 2.15 | 40,938 | 98,325 |
| XDNS-58 | 58 | 54.43 | 5.08 | 1.93 | 55 | 2.15 | 42,400 | 101,836 |
| XDNS-60 | 60 | 56.42 | 5.08 | 1.93 | 57 | 2.15 | 43,863 | 105,348 |
| XDNS-62 | 62 | 58.42 | 5.08 | 1.93 | 59 | 2.15 | 45,325 | 108,860 |
| XDNS-63 | 63 | 59.39 | 5.08 | 1.93 | 60 | 2.15 | 46,056 | 110,615 |
| XDNS-65 | 65 | 61.39 | 5.08 | 2.41 | 62 | 2.65 | 47,518 | 135,725 |
| XDNS-67 | 67 | 63.37 | 5.08 | 2.41 | 64 | 2.65 | 48,980 | 139,901 |
| XDNS-68 | 68 | 64.34 | 5.08 | 2.41 | 65 | 2.65 | 49,711 | 141,989 |
| XDNS-70 | 70 | 66.34 | 5.08 | 2.41 | 67 | 2.65 | 51,173 | 146,165 |
| XDNS-72 | 72 | 68.33 | 5.08 | 2.41 | 69 | 2.65 | 52,635 | 150,341 |
| XDNS-75 | 75 | 71.33 | 5.08 | 2.41 | 72 | 2.65 | 54,828 | 156,605 |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |