Metric Slotted Raised Countersunk Head Self Tapping Screw AB Stainless-Steel-A2 DIN7973C

SKU: 465
Details
Details
Metric Slotted Raised Countersunk Head Self Tapping Screw AB Stainless-Steel-A2 DIN7973C
dadk maxk maxftbyl minl max
ST 2.20.80004.30001.30000.50000.80000.50002.00004.500016.0000
ST 2.91.10005.50001.70000.70001.20000.80002.60006.500019.0000
ST 3.51.30006.80002.10000.80001.40001.00003.20009.500025.0000
ST 4.21.40008.10002.50001.00001.60001.20003.70009.500032.0000
ST 4.81.60009.50003.00001.20002.00001.20004.30009.500032.0000
ST 5.51.800010.80003.40001.30002.20001.60005.000013.000038.0000
ST 6.31.800012.40003.80001.40002.40001.60006.000013.000038.0000
ST82.1000--2.00003.20002.00007.500016.000050.0000
ST 9.52.1000--2.30003.80002.50008.000019.000050.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN7973C
Second StandardISO1483
DriveSlot
HeadRaisedcountersunk
American Generic Brand TermFLAT
Diameter ST2.2,ST2.9,ST3.5,ST3.9,ST4.2,ST4.8,ST5.5,ST6.3,ST8,ST9.5
Length4.5,6.5,9.5,13,16,19,25,30,32,38,50