d1k maxd2 maxa maxy Bl minl max
ST 2.21.80004.20000.80001.60004.500016.0000
ST 2.92.20005.60001.10002.10006.500019.0000
ST 3.52.60006.90001.30002.50009.500025.0000
ST 3.92.80007.50001.3000 9.500030.0000
ST 4.23.05008.20001.40002.80009.500032.0000
ST 4.83.55009.50001.60003.20009.500038.0000
ST 5.53.950010.80001.80003.600013.000038.0000
ST 6.34.550012.50001.80003.600013.000038.0000
ST 85.250015.80002.10004.200016.000050.0000
ST 9.5  2.10004.200019.000050.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN7981FH
Second StandardISO7049
DrivePhillips
HeadPan
American Generic Brand Term-
Diameter ST2.2,ST2.9,ST3.5,ST3.9,ST4.2,ST4.8,ST5.5,ST6.3,ST8,ST9.5
Length4.5,6.5,9.5,13,16,19,25,30,32,38,50