Metric Flat Washer For Sems Self Tapping Screws Type N Steel-100Hv ISO10644
SKU:
2299
Details
Details
Metric Flat Washer For Sems Self Tapping Screws Type N Steel-100Hv ISO10644
| d | d1 min | d1 max | d2 max | d2 min | h nom | h max | h min |
|---|
| 2.2 | 1.9000 | 2.0000 | 5.0000 | 4.8200 | 1.0000 | 1.0600 | 0.9400 |
| 2.9 | 2.5000 | 2.6000 | 7.0000 | 6.6400 | 1.0000 | 1.0600 | 0.9400 |
| 3.5 | 3.0000 | 3.1000 | 8.0000 | 7.6400 | 1.0000 | 1.0600 | 0.9400 |
| 4.2 | 3.5500 | 3.6700 | 9.0000 | 8.6400 | 1.0000 | 1.0600 | 0.9400 |
| 4.8 | 4.0000 | 4.1200 | 10.0000 | 9.6400 | 1.0000 | 1.0600 | 0.9400 |
| 5.5 | 4.7000 | 4.8200 | 12.0000 | 11.5700 | 1.6000 | 1.0600 | 1.5200 |
| 6.3 | 5.4000 | 5.5200 | 14.0000 | 13.5700 | 1.6000 | 1.6800 | 1.5200 |
| 8 | 7.1500 | 7.3000 | 16.0000 | 15.5700 | 1.6000 | 1.6800 | 1.5200 |
| 9.5 | 8.8000 | 8.9500 | 20.0000 | 19.4800 | 2.0000 | 2.0900 | 1.9100 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Steel-100Hv |
|---|
| Standard Number | ISO10644 |
|---|
| Second Standard | - |
|---|
| Drive | Various |
|---|
| Head | Various |
|---|
| American Generic Brand Term | SEMS |
|---|
| Diameter | 2.20,2.90,3.50,4.20,4.80,5.50,6.30,8.00,9.50 |
|---|
| Length | NON |
|---|