sizep minp maxd mind maxa mina maxh minh maxs nomhole minhole maxdrill
1.41.35001.40001.53001.63002.20002.60000.35000.55001.00001.40001.46001.4000
1.61.55001.60001.73001.83002.60003.00000.45000.65001.00001.60001.66001.6000
21.95002.00002.20002.30003.30003.70000.55000.75001.00002.00002.06002.0000
2.52.45002.50002.70002.80004.20004.60000.70000.90001.00002.50002.56002.5000
32.95003.00003.25003.35004.95005.45000.90001.20001.00003.00003.06003.0000
43.95004.00004.25004.35006.75007.25001.20001.50002.00004.00004.08004.0000
54.95005.00005.25005.35008.50009.10001.50001.80002.00005.00005.08005.0000
65.95006.00006.25006.350010.200010.80001.90002.20002.00006.00006.08006.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second Standard-
DriveNon
HeadFlat
American Generic Brand Term-
Diameter 1.4,1.6,2,2.5,3,4,5,6
Length5,6,8,10,12,16,20