Metric Fine pitch Nylon Insert Flange Self Locking Nut Class-10 DIN6926
Metric Fine Pitch Nylon Insert Flange Self Locking Nut Class-10 DIN6926 din 6926
D | d2 | h | m | s |
---|---|---|---|---|
M5 | 11.8000 | 7.1000 | 4.7000 | 8.0000 |
M6 | 14.2000 | 9.1000 | 5.7000 | 10.0000 |
M8 | 17.9000 | 11.1000 | 7.6000 | 13.0000 |
M10 | 21.8000 | 13.5000 | 9.6000 | 15.0000 |
M12 | 26.0000 | 16.1000 | 11.6000 | 18.0000 |
M14 | 29.9000 | 18.2000 | 13.3000 | 21.0000 |
M16 | 34.5000 | 20.3000 | 15.3000 | 24.0000 |
M20 | 42.8000 | 24.8000 | 18.9000 | 30.0000 |
Weight | 0.0000 |
---|---|
Material | Class-8 |
Standard Number | DIN6926 |
Second Standard | ISO7043 |
Drive | Hexagon |
Head | NON |
American Generic Brand Term | STIFF,PREVAILINGTORQUE |
Diameter | M5,M6M8,M10,M12,M14,M16,M20 |
Length | NON |