dds maxds minS nomS minE minK nomK maxK min
M1.61.60001.46003.20003.02003.41001.10001.22500.9750
M22.00001.86004.00003.82004.32001.40001.52501.2750
M2.52.50002.36005.00004.82005.45001.70001.82501.5750
M33.00002.86005.50005.32006.01002.00002.12501.8750
M44.00003.82007.00006.78007.66002.80002.92502.6750
M55.00004.82008.00007.78008.79003.50003.65003.3500
M66.00005.820010.00009.780011.05004.00004.15003.8500
M88.00007.780013.000012.730014.38005.30005.45005.1500
M1010.00009.780016.000015.730017.77006.40006.58006.2200
M1212.000011.730018.000017.730020.03007.50007.68007.3200
M1616.000015.730024.000023.670026.750010.000010.18009.8200
M2020.000019.670030.000029.670033.530012.500012.715012.2850
M2424.000023.670036.000035.380039.980015.000015.215014.7850
M3030.000029.480046.000045.000050.850018.7000 - -
M3636.000035.380055.000053.800060.790022.5000 - -
M4242.000041.380065.000063.100071.300026.0000 - -
M4848.000047.380075.000073.100082.600030.0000 - -
M5656.000055.260085.000082.800093.560035.0000 - -
M6464.000063.260095.000092.8000104.860040.0000 - -
Additional Info
Additional Info
Weight0.0000
MaterialGrade-8.8
Standard NumberISO4014
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand TermHEXAGONCAP
Diameter M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M7,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39,M42,M45,M48,M52,M56,M60,M64
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300,320,340,350,360,380,400,420,440,460,480,500