Metric Coarse Elevator Bucket Bolt Grade-3.6 DIN15237

SKU: 224
Details
Details

Metric Coarse Elevator Bucket Bolt Grade-3.6 DIN15237

dkgad3
M62.50003.500014.000020.0000
M83.50005.000020.000028.0000
M 104.50006.000025.000035.0000
M 125.20007.000030.000042.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-3.6
Standard NumberDIN15237
Second Standard-
DriveNon
HeadDish
American Generic Brand TermSEATING SCREW
Diameter M6,M7,M8,M10,M12
Length20,22,24,26,28,30,35,40,45,50,55,60,65,70