Metric Coarse Double Nib Tee Slot Bolt Stainless-Steel-A2 DIN188

SKU: 199
Details
Details
Metric Coarse Double Nib Tee Slot Bolt Stainless-Steel-A2 DIN188
d b k m n
M822.00005.500018.00008.0000
M1026.00007.000021.000010.0000
M1230.00008.000026.000012.0000
M1638.000010.500030.000016.0000
M2046.000013.000036.500020.0000
M2454.000015.000043.000024.0000
M3066.000019.000054.000030.0000
M3678.000022.000066.000035.5000
M4296.000026.000080.000042.2500
M48108.000030.000088.000048.5000
M56124.000035.0000101.750056.0000
M64130.000040.5000115.000064.0000
M72158.000045.5000128.000072.2500
M80172.000049.5000140.000080.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN188
Second Standard-
DriveNon
HeadTEE
American Generic Brand TermT'
Diameter M8,M10,M12,M16,M20,M24,M30,M36,M42,M48,M56,M64,M72,M80
Length30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300,320,340,350,360,380,400