Metric Coarse Centre Locking Thin Jam Nut Steel class 4
Metric Coarse Centre Locking Jam Nut Steel Class 4
can be installed from either direction
| d | s | e | m |
|---|---|---|---|
| M6 | 10.0000 | 11.0500 | 3.2000 |
| M8 | 13.0000 | 14.3800 | 4.0000 |
| M10 | 17.0000 | 18.9000 | 5.0000 |
| M12 | 19.0000 | 21.1000 | 6.0000 |
| M14 | 22.0000 | 24.4900 | 7.0000 |
| M16 | 24.0000 | 26.7500 | 8.0000 |
| M18 | 27.0000 | 29.5600 | 9.0000 |
| M20 | 30.0000 | 32.9500 | 10.0000 |
| M22 | 32.0000 | 35.0300 | 11.0000 |
| M24 | 36.0000 | 39.5500 | 12.0000 |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |