Metric Coarse 12 Point Spline Bell Flange Head Bolt Grade-8.8 B18.2.7.1M

SKU: 110
Details
Details
Metric Coarse 12 Point Spline Bell Flange Head Bolt Grade-8.8 B18.2.7.1M
Dbds maxds mindc maxk max
M516.00005.00004.82009.40005.0000
M618.00006.00005.820011.30006.0000
M822.00008.00007.780015.00008.0000
M1026.000010.00009.780018.600010.0000
M1230.000012.000011.730022.800012.0000
M1434.000014.000013.730026.400014.0000
M1638.000016.000015.730030.300016.0000
M2046.000020.000019.670037.400020.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-8.8
Standard NumberB18.2.7.1M
Second Standard-
Drive12point
HeadFlange
American Generic Brand Term SPLINE,FERRY,BELL
Diameter M5,M6,M8,M10,M12,M14,M16,M20
Length16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100