Internal Spirolox Retaining Rings Type XWHM Heavy Duty Inch
Internal Spirolox Retaining Rings Type XWHM Heavy Duty Inch
The WHM Series Spirolox Retaining Ring is designed for the toughest retaining ring jobs. WHM series retaining rings use standard industry groove dimensions and are interchangeable with many stamped retaining rings. This series should be specified for thrust loads that demand deep groove, heavy section capacity.
Standard Parts:
1/4"-15" Diameters
Standard Materials:
Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel
| Part Number | Housing Diameter | Ring Outside Diameter | Ring Radial Wall | Ring Thickness | Groove Diameter | Groove Width | Groove Yield (1) | Ring Shear (2) |
| XWHM-25* | 0.250 | 0.270 | 0.020 | 0.015 | 0.268 | 0.020 | 159 | 561 |
| XWHM-31* | 0.312 | 0.333 | 0.025 | 0.015 | 0.330 | 0.020 | 198 | 700 |
| XWHM-37* | 0.375 | 0.400 | 0.030 | 0.025 | 0.397 | 0.029 | 292 | 1,442 |
| XWHM-43 | 0.437 | 0.464 | 0.035 | 0.025 | 0.461 | 0.029 | 371 | 1,680 |
| XWHM-50 | 0.500 | 0.538 | 0.045 | 0.035 | 0.530 | 0.039 | 530 | 2,530 |
| XWHM-51 | 0.512 | 0.550 | 0.045 | 0.035 | 0.542 | 0.039 | 540 | 2,590 |
| XWHM-56 | 0.562 | 0.605 | 0.055 | 0.035 | 0.596 | 0.039 | 680 | 2,840 |
| XWHM-62 | 0.625 | 0.675 | 0.055 | 0.035 | 0.665 | 0.039 | 880 | 3,160 |
| XWHM-68 | 0.688 | 0.743 | 0.065 | 0.035 | 0.732 | 0.039 | 1,070 | 3,480 |
| XWHM-75 | 0.750 | 0.807 | 0.065 | 0.035 | 0.796 | 0.039 | 1,220 | 3,790 |
| XWHM-77 | 0.777 | 0.836 | 0.075 | 0.042 | 0.825 | 0.046 | 1,320 | 4,720 |
| XWHM-81 | 0.812 | 0.873 | 0.075 | 0.042 | 0.862 | 0.046 | 1,440 | 4,930 |
| XWHM-86 | 0.866 | 0.931 | 0.075 | 0.042 | 0.920 | 0.046 | 1,650 | 5,260 |
| XWHM-87 | 0.875 | 0.943 | 0.085 | 0.042 | 0.931 | 0.046 | 1,730 | 5,310 |
| XWHM-90 | 0.901 | 0.972 | 0.085 | 0.042 | 0.959 | 0.046 | 1,850 | 5,470 |
| XWHM-93 | 0.938 | 1.013 | 0.085 | 0.042 | 1.000 | 0.046 | 2,060 | 5,690 |
| XWHM-100 | 1.000 | 1.080 | 0.085 | 0.042 | 1.066 | 0.046 | 2,330 | 6,070 |
| XWHM-102 | 1.023 | 1.105 | 0.085 | 0.042 | 1.091 | 0.046 | 2,460 | 6,210 |
| XWHM-106 | 1.062 | 1.138 | 0.103 | 0.050 | 1.130 | 0.056 | 2,550 | 7,010 |
| XWHM-112 | 1.125 | 1.205 | 0.103 | 0.050 | 1.197 | 0.056 | 2,860 | 7,420 |
| XWHM-118 | 1.188 | 1.271 | 0.103 | 0.050 | 1.262 | 0.056 | 3,110 | 7,840 |
| XWHM-125 | 1.250 | 1.339 | 0.103 | 0.050 | 1.330 | 0.056 | 3,530 | 8,250 |
| XWHM-131 | 1.312 | 1.406 | 0.118 | 0.050 | 1.396 | 0.056 | 3,900 | 8,660 |
| XWHM-137 | 1.375 | 1.471 | 0.118 | 0.050 | 1.461 | 0.056 | 4,180 | 9,070 |
| XWHM-143 | 1.439 | 1.539 | 0.118 | 0.050 | 1.528 | 0.056 | 4,580 | 9,490 |
| XWHM-145 | 1.456 | 1.559 | 0.118 | 0.050 | 1.548 | 0.056 | 4,730 | 9,610 |
| XWHM-150 | 1.500 | 1.605 | 0.118 | 0.050 | 1.594 | 0.056 | 4,980 | 9,900 |
| XWHM-156 | 1.562 | 1.675 | 0.128 | 0.062 | 1.658 | 0.068 | 5,300 | 12,780 |
| XWHM-162 | 1.625 | 1.742 | 0.128 | 0.062 | 1.725 | 0.068 | 5,740 | 13,290 |
| XWHM-165 | 1.653 | 1.772 | 0.128 | 0.062 | 1.755 | 0.068 | 5,960 | 13,520 |
| XWHM-168 | 1.688 | 1.810 | 0.128 | 0.062 | 1.792 | 0.068 | 6,210 | 13,810 |
| XWHM-175 | 1.750 | 1.876 | 0.128 | 0.062 | 1.858 | 0.068 | 6,680 | 14,320 |
| XWHM-181 | 1.812 | 1.940 | 0.128 | 0.062 | 1.922 | 0.068 | 7,050 | 14,820 |
| XWHM-185 | 1.850 | 1.981 | 0.158 | 0.062 | 1.962 | 0.068 | 7,320 | 15,130 |
| XWHM-187 | 1.875 | 2.008 | 0.158 | 0.062 | 1.989 | 0.068 | 7,560 | 15,340 |
| XWHM-193 | 1.938 | 2.075 | 0.158 | 0.062 | 2.056 | 0.068 | 8,080 | 15,850 |
| XWHM-200 | 2.000 | 2.142 | 0.158 | 0.062 | 2.122 | 0.068 | 8,620 | 16,360 |
| XWHM-206 | 2.062 | 2.201 | 0.168 | 0.078 | 2.186 | 0.086 | 9,040 | 21,220 |
| XWHM-212 | 2.125 | 2.267 | 0.168 | 0.078 | 2.251 | 0.086 | 9,460 | 21,870 |
| XWHM-218 | 2.188 | 2.334 | 0.168 | 0.078 | 2.318 | 0.086 | 10,050 | 22,520 |
| XWHM-225 | 2.250 | 2.399 | 0.168 | 0.078 | 2.382 | 0.086 | 10,500 | 23,160 |
| XWHM-231 | 2.312 | 2.467 | 0.200 | 0.078 | 2.450 | 0.086 | 11,280 | 23,800 |
| XWHM-237 | 2.375 | 2.535 | 0.200 | 0.078 | 2.517 | 0.086 | 11,920 | 24,440 |
| XWHM-244 | 2.440 | 2.602 | 0.200 | 0.078 | 2.584 | 0.086 | 12,420 | 25,110 |
| XWHM-250 | 2.500 | 2.667 | 0.200 | 0.078 | 2.648 | 0.086 | 13,080 | 25,730 |
| XWHM-253 | 2.531 | 2.700 | 0.200 | 0.078 | 2.681 | 0.086 | 13,420 | 26,050 |
| XWHM-256 | 2.562 | 2.733 | 0.225 | 0.093 | 2.714 | 0.103 | 13,760 | 29,940 |
| XWHM-262 | 2.625 | 2.801 | 0.225 | 0.093 | 2.781 | 0.103 | 14,470 | 30,680 |
| XWHM-268 | 2.688 | 2.868 | 0.225 | 0.093 | 2.848 | 0.103 | 15,200 | 31,410 |
| XWHM-275 | 2.750 | 2.934 | 0.225 | 0.093 | 2.914 | 0.103 | 15,940 | 32,140 |
| XWHM-281 | 2.813 | 3.001 | 0.225 | 0.093 | 2.980 | 0.103 | 16,700 | 32,880 |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |