sizesizeA maxA minB maxB minc maxc min
No.4       0.112       0.123       0.115       0.510       0.495       0.021       0.017
No.6       0.138       0.150       0.141       0.610       0.580       0.028       0.023
No.8       0.164       0.176       0.168       0.690       0.670       0.034       0.028
No.10       0.190       0.204       0.195       0.690       0.670       0.040       0.032
No.12       0.216       0.231       0.221       0.760       0.725       0.040       0.032
1/4"       0.250       0.267       0.256       0.900       0.880       0.040       0.032
5/16"       0.312       0.332       0.320       0.985       0.965       0.045       0.037
3/8"       0.375       0.398       0.384       1.070       1.045       0.050       0.042
7/16"       0.438       0.464       0.448       1.155       1.130       0.050       0.042
1/2"       0.500       0.530       0.512       1.315       1.290       0.055       0.047
9/16"       0.562       0.596       0.576       1.430       1.380       0.060       0.052
5/8"       0.625       0.663       0.640       1.620       1.590       0.067       0.059

 

Inch Internal External Toothed Shake proof Washer Spring Steel  B18.21.1 T10

Additional Info
Additional Info
Weight0.0000
MaterialSpring-Steel
Standard NumberB18.2.1.1T10
Second Standard-
DriveNon
HeadNON
American Generic Brand TermLOCKWASHER
Diameter0
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.