Smalley Single Turn Wave Spring Inch Steel
Smalley Single Turn Wave Spring Inch Steel
Conventional Gap and Overlap Type Wave Springs are used in a wide variety of applications. For short deflections and low-medium forces, they function with precision and dependability.
These two types of Smalley Wave Springs permit radial expansion or growth in diameter within a cavity, without the binding or hang-up normally associated with die stamped wave washers. Just as their terms imply, the gap type is split to retain a gap between the ends, while the overlap type has overlapping ends. Thus, the ends are free to move circumferentially as the spring outside diameter grows during compression.

| Part Number | Operates in a bore dia. | Clears Shaft dia. | Load (lb) | Work Height | Reference Free Height | No of Waves | Thickness | Radial Wall | Reference Spring Rate (lb/in) | Type |
| YSSR-0050 | 0.500 | 0.39 | 7 | 0.050 | 0.085 | 3 | 0.008 | 0.040 | 200 | overlap |
| YSSR-0062 | 0.625 | 0.48 | 10 | 0.050 | 0.095 | 3 | 0.010 | 0.058 | 222 | overlap |
| YSSR-0075 | 0.750 | 0.50 | 14 | 0.062 | 0.160 | 3 | 0.010 | 0.078 | 143 | overlap |
| YSSR-0087 | 0.875 | 0.62 | 16 | 0.062 | 0.130 | 3 | 0.012 | 0.094 | 235 | overlap |
| YSSR-0100 | 1.000 | 0.78 | 18 | 0.062 | 0.160 | 3 | 0.012 | 0.094 | 184 | overlap |
| YSSR-0112 | 1.125 | 0.84 | 20 | 0.078 | 0.130 | 3 | 0.016 | 0.133 | 385 | overlap |
| YSSR-0125 | 1.250 | 0.96 | 22 | 0.078 | 0.150 | 3 | 0.016 | 0.133 | 306 | overlap |
| YSSR-0137 | 1.375 | 1.09 | 24 | 0.078 | 0.190 | 3 | 0.016 | 0.133 | 214 | overlap |
| YSSR-0150 | 1.500 | 1.17 | 26 | 0.078 | 0.170 | 3 | 0.018 | 0.143 | 283 | overlap |
| YSSR-0162 | 1.625 | 1.31 | 28 | 0.078 | 0.200 | 3 | 0.018 | 0.143 | 230 | overlap |
| YSSR-0175 | 1.750 | 1.44 | 30 | 0.078 | 0.140 | 4 | 0.018 | 0.143 | 484 | gap |
| YSSR-0187 | 1.875 | 1.56 | 32 | 0.078 | 0.150 | 4 | 0.018 | 0.143 | 444 | gap |
| YSSR-0200 | 2.000 | 1.68 | 34 | 0.093 | 0.140 | 4 | 0.024 | 0.150 | 723 | gap |
| YSSR-0212 | 2.125 | 1.80 | 36 | 0.093 | 0.150 | 4 | 0.024 | 0.150 | 632 | gap |
| YSSR-0225 | 2.250 | 1.93 | 38 | 0.093 | 0.170 | 4 | 0.024 | 0.150 | 494 | gap |
| YSSR-0237 | 2.375 | 1.99 | 40 | 0.093 | 0.160 | 4 | 0.024 | 0.178 | 597 | gap |
| YSSR-0250 | 2.500 | 2.12 | 42 | 0.093 | 0.170 | 4 | 0.024 | 0.178 | 545 | gap |
| YSSR-0262 | 2.625 | 2.24 | 44 | 0.093 | 0.190 | 4 | 0.024 | 0.178 | 454 | gap |
| YSSR-0275 | 2.750 | 2.34 | 46 | 0.109 | 0.170 | 4 | 0.030 | 0.188 | 754 | gap |
| YSSR-0287 | 2.875 | 2.47 | 48 | 0.109 | 0.180 | 4 | 0.030 | 0.188 | 676 | gap |
| YSSR-0300 | 3.000 | 2.59 | 50 | 0.109 | 0.190 | 4 | 0.030 | 0.188 | 617 | gap |
| YSSR-0312 | 3.125 | 2.71 | 52 | 0.109 | 0.210 | 4 | 0.030 | 0.188 | 515 | gap |
| YSSR-0325 | 3.250 | 2.75 | 54 | 0.109 | 0.200 | 4 | 0.030 | 0.233 | 593 | gap |
| YSSR-0337 | 3.375 | 2.84 | 56 | 0.109 | 0.220 | 4 | 0.030 | 0.233 | 505 | gap |
| YSSR-0350 | 3.500 | 3.00 | 58 | 0.109 | 0.230 | 4 | 0.030 | 0.233 | 479 | gap |
| YSSR-0362 | 3.625 | 3.12 | 60 | 0.109 | 0.240 | 4 | 0.030 | 0.233 | 458 | gap |
| YSSR-0375 | 3.750 | 3.25 | 62 | 0.109 | 0.260 | 4 | 0.030 | 0.233 | 411 | gap |
| YSSR-0387 | 3.875 | 3.37 | 64 | 0.109 | 0.300 | 4 | 0.030 | 0.233 | 335 | gap |
| YSSR-0400 | 4.000 | 3.50 | 66 | 0.109 | 0.190 | 5 | 0.030 | 0.233 | 815 | gap |
| YSSR-0412 | 4.125 | 3.62 | 67 | 0.109 | 0.200 | 5 | 0.030 | 0.233 | 736 | gap |
| YSSR-0425 | 4.250 | 3.74 | 69 | 0.109 | 0.210 | 5 | 0.030 | 0.233 | 683 | gap |
| YSSR-0437 | 4.375 | 3.86 | 70 | 0.109 | 0.210 | 5 | 0.030 | 0.233 | 693 | gap |
| YSSR-0450 | 4.500 | 3.99 | 72 | 0.109 | 0.230 | 5 | 0.030 | 0.233 | 595 | gap |
| YSSR-0462 | 4.625 | 4.11 | 73 | 0.125 | 0.270 | 5 | 0.030 | 0.233 | 503 | gap |
| YSSR-0475 | 4.750 | 4.24 | 75 | 0.125 | 0.310 | 5 | 0.030 | 0.233 | 405 | gap |
| YSSR-0487 | 4.875 | 4.37 | 76 | 0.125 | 0.290 | 5 | 0.030 | 0.233 | 461 | gap |
| YSSR-0500 | 5.000 | 4.49 | 78 | 0.125 | 0.310 | 5 | 0.030 | 0.233 | 422 | gap |
| YSSR-0512 | 5.125 | 4.61 | 80 | 0.125 | 0.340 | 5 | 0.030 | 0.233 | 372 | gap |
| YSSR-0525 | 5.250 | 4.74 | 82 | 0.125 | 0.370 | 5 | 0.030 | 0.233 | 335 | gap |
| YSSR-0537 | 5.375 | 4.86 | 84 | 0.125 | 0.380 | 5 | 0.030 | 0.233 | 329 | gap |
| YSSR-0550 | 5.500 | 4.99 | 86 | 0.125 | 0.250 | 6 | 0.030 | 0.233 | 688 | gap |
| YSSR-0562 | 5.625 | 5.11 | 88 | 0.125 | 0.270 | 6 | 0.030 | 0.233 | 607 | gap |
| YSSR-0575 | 5.750 | 5.24 | 90 | 0.125 | 0.280 | 6 | 0.030 | 0.233 | 581 | gap |
| YSSR-0587 | 5.875 | 5.36 | 92 | 0.125 | 0.300 | 6 | 0.030 | 0.233 | 526 | gap |
| YSSR-0600 | 6.000 | 5.49 | 94 | 0.125 | 0.300 | 6 | 0.030 | 0.233 | 537 | gap |
| YSSR-0612 | 6.125 | 5.61 | 96 | 0.125 | 0.310 | 6 | 0.030 | 0.233 | 519 | gap |
| YSSR-0625 | 6.250 | 5.73 | 98 | 0.125 | 0.340 | 6 | 0.030 | 0.233 | 456 | gap |
| YSSR-0637 | 6.375 | 5.86 | 100 | 0.125 | 0.350 | 6 | 0.030 | 0.233 | 444 | gap |
| YSSR-0650 | 6.500 | 5.98 | 102 | 0.125 | 0.390 | 6 | 0.030 | 0.233 | 385 | gap |
| YSSR-0675 | 6.750 | 6.23 | 104 | 0.125 | 0.420 | 6 | 0.030 | 0.233 | 353 | gap |
| YSSR-0700 | 7.000 | 6.16 | 106 | 0.156 | 0.320 | 6 | 0.032 | 0.375 | 646 | gap |
| YSSR-0725 | 7.250 | 6.44 | 108 | 0.156 | 0.350 | 6 | 0.032 | 0.375 | 557 | gap |
| YSSR-0750 | 7.500 | 6.69 | 110 | 0.156 | 0.360 | 6 | 0.032 | 0.375 | 539 | gap |
| YSSR-0775 | 7.750 | 6.94 | 114 | 0.156 | 0.380 | 6 | 0.032 | 0.375 | 509 | gap |
| YSSR-0800 | 8.000 | 7.19 | 118 | 0.156 | 0.390 | 6 | 0.032 | 0.375 | 504 | gap |
| YSSR-0825 | 8.250 | 7.44 | 122 | 0.156 | 0.430 | 6 | 0.032 | 0.375 | 445 | gap |
| YSSR-0850 | 8.500 | 7.68 | 126 | 0.156 | 0.340 | 7 | 0.032 | 0.375 | 685 | gap |
| YSSR-0875 | 8.750 | 7.93 | 130 | 0.156 | 0.340 | 7 | 0.032 | 0.375 | 707 | gap |
| YSSR-0900 | 9.000 | 8.18 | 134 | 0.156 | 0.290 | 8 | 0.032 | 0.375 | 1,000 | gap |
| YSSR-0950 | 9.500 | 8.68 | 142 | 0.156 | 0.240 | 9 | 0.032 | 0.375 | 1,690 | gap |
| YSSR-1000 | 10.000 | 9.17 | 150 | 0.156 | 0.290 | 9 | 0.032 | 0.375 | 1,119 | gap |
| YSSR-1050 | 10.500 | 9.67 | 158 | 0.156 | 0.310 | 9 | 0.032 | 0.375 | 1,026 | gap |
| YSSR-1100 | 11.000 | 10.17 | 166 | 0.156 | 0.350 | 9 | 0.032 | 0.375 | 856 | gap |
| YSSR-1150 | 11.500 | 10.66 | 174 | 0.156 | 0.360 | 9 | 0.032 | 0.375 | 853 | gap |
| YSSR-1200 | 12.000 | 11.16 | 182 | 0.156 | 0.440 | 9 | 0.032 | 0.375 | 641 | gap |
| YSSR-1250 | 12.500 | 11.66 | 190 | 0.156 | 0.350 | 10 | 0.032 | 0.375 | 979 | gap |
| YSSR-1300 | 13.000 | 12.16 | 198 | 0.156 | 0.410 | 10 | 0.032 | 0.375 | 780 | gap |
| YSSR-1350 | 13.500 | 12.65 | 206 | 0.156 | 0.430 | 10 | 0.032 | 0.375 | 752 | gap |
| YSSR-1400 | 14.000 | 13.15 | 214 | 0.156 | 0.300 | 12 | 0.032 | 0.375 | 1,486 | gap |
| YSSR-1450 | 14.500 | 13.65 | 221 | 0.156 | 0.320 | 12 | 0.032 | 0.375 | 1,348 | gap |
| YSSR-1500 | 15.000 | 14.13 | 230 | 0.156 | 0.350 | 12 | 0.032 | 0.375 | 1,186 | gap |
| YSSR-1550 | 15.500 | 14.64 | 239 | 0.156 | 0.310 | 13 | 0.032 | 0.375 | 1,552 | gap |
| YSSR-1600 | 16.000 | 15.14 | 248 | 0.156 | 0.340 | 13 | 0.032 | 0.375 | 1,348 | gap |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |