Smalley Single Turn Bearing Preload Spring Steel
Smalley Single Turn Bearing Preload Spring Steel
Smalley Circular-Grain bearing preload Wave Springs eliminate play and minimize bearing noise. The constant light/medium pressure they apply removes play between the ball bearings and the bearings’ inner and outer races. Preloading can reduce the possibility of bearing damage due to vibration (vibratory loading) and wear due to repetitive and non-repetitive run out.


| Part Number | Bearing OD (1) | Clears Shaft dia. | Load (N) | Work Height | Reference Free Height | No of Waves | Thickness | Radial Wall | Reference Spring Rate (N/mm) | Type |
| YSSB-0063 | 16 | 11.28 | 44.5 | 1.57 | 2.29 | 3 | 0.25 | 1.98 | 65 | overlap |
| YSSB-0075 | 19 | 14.28 | 53.4 | 1.57 | 3.05 | 3 | 0.25 | 1.98 | 35 | overlap |
| YSSB-0087 | 22 | 16.46 | 62.3 | 1.57 | 2.79 | 3 | 0.3 | 2.39 | 48 | overlap |
| YSSB-0095 | 24 | 18.46 | 66.7 | 1.57 | 3.56 | 3 | 0.3 | 2.39 | 35 | overlap |
| YSSB-0102 | 26 | 18.22 | 71.2 | 1.98 | 2.54 | 3 | 0.41 | 3.38 | 111 | overlap |
| YSSB-0110 | 28 | 20.22 | 75.6 | 1.98 | 2.79 | 3 | 0.41 | 3.38 | 85 | overlap |
| YSSB-0118 | 30 | 22.22 | 84.5 | 1.98 | 3.3 | 3 | 0.41 | 3.38 | 66 | overlap |
| YSSB-0126 | 32 | 24.22 | 89 | 1.98 | 3.81 | 3 | 0.41 | 3.38 | 52 | overlap |
| YSSB-0138 | 35 | 27.22 | 97.9 | 1.98 | 4.57 | 3 | 0.41 | 3.38 | 38 | overlap |
| YSSB-0146 | 37 | 28.72 | 102.3 | 1.98 | 3.81 | 3 | 0.46 | 3.63 | 58 | overlap |
| YSSB-0158 | 40 | 31.72 | 111.2 | 1.98 | 5.08 | 3 | 0.46 | 3.63 | 37 | overlap |
| YSSB-0165 | 42 | 33.72 | 115.7 | 1.98 | 3.05 | 4 | 0.46 | 3.63 | 99 | overlap |
| YSSB-0185 | 47 | 38.72 | 129 | 1.98 | 3.81 | 4 | 0.46 | 3.63 | 68 | overlap |
| YSSB-0205 | 52 | 43.11 | 142.4 | 2.36 | 3.56 | 4 | 0.61 | 3.76 | 121 | overlap |
| YSSB-0217 | 55 | 46.11 | 151.3 | 2.36 | 3.81 | 4 | 0.61 | 3.76 | 100 | overlap |
| YSSB-0244 | 62 | 51.69 | 169.1 | 2.36 | 4.32 | 4 | 0.61 | 4.52 | 85 | overlap |
| YSSB-0268 | 68 | 57.17 | 186.9 | 2.77 | 4.32 | 4 | 0.76 | 4.78 | 131 | overlap |
| YSSB-0276 | 70 | 59.17 | 191.3 | 2.77 | 4.32 | 4 | 0.76 | 4.78 | 119 | overlap |
| YSSB-0284 | 72 | 61.17 | 195.8 | 2.77 | 4.57 | 4 | 0.76 | 4.78 | 108 | overlap |
| YSSB-0295 | 75 | 64.17 | 204.7 | 2.77 | 5.08 | 4 | 0.76 | 4.78 | 94 | overlap |
| YSSB-0315 | 80 | 68.66 | 218 | 2.77 | 5.59 | 4 | 0.76 | 4.78 | 76 | overlap |
| YSSB-0335 | 85 | 71.38 | 231.4 | 2.77 | 5.59 | 4 | 0.76 | 5.92 | 83 | overlap |
| YSSB-0354 | 90 | 76.38 | 249.2 | 2.77 | 6.35 | 4 | 0.76 | 5.92 | 68 | overlap |
| YSSB-0374 | 95 | 81.38 | 262.5 | 2.77 | 7.37 | 4 | 0.76 | 5.92 | 57 | overlap |
| YSSB-0394 | 100 | 86.38 | 275.9 | 2.77 | 4.57 | 5 | 0.76 | 5.92 | 157 | gap |
| YSSB-0413 | 105 | 91.38 | 289.2 | 2.77 | 5.08 | 5 | 0.76 | 5.92 | 134 | gap |
| YSSB-0433 | 110 | 96.38 | 302.6 | 2.77 | 5.33 | 5 | 0.76 | 5.92 | 115 | gap |
| YSSB-0453 | 115 | 101.38 | 315.9 | 3.18 | 6.35 | 5 | 0.76 | 5.92 | 99 | gap |
| YSSB-0472 | 120 | 106.38 | 329.3 | 3.18 | 7.11 | 5 | 0.76 | 5.92 | 86 | gap |
| YSSB-0492 | 125 | 111.38 | 342.6 | 3.18 | 7.62 | 5 | 0.76 | 5.92 | 76 | gap |
| YSSB-0512 | 130 | 116.38 | 356 | 3.18 | 8.64 | 5 | 0.76 | 5.92 | 67 | gap |
| YSSB-0532 | 135 | 121.38 | 369.3 | 3.18 | 9.4 | 5 | 0.76 | 5.92 | 59 | gap |
| YSSB-0551 | 140 | 126.38 | 382.7 | 3.18 | 6.86 | 6 | 0.76 | 5.92 | 108 | gap |
| YSSB-0571 | 145 | 131.38 | 396 | 3.18 | 7.37 | 6 | 0.76 | 5.92 | 97 | gap |
| YSSB-0591 | 150 | 136.38 | 404.9 | 3.18 | 7.87 | 6 | 0.76 | 5.92 | 87 | gap |
| YSSB-0630 | 160 | 146.38 | 440.5 | 3.18 | 9.4 | 6 | 0.76 | 5.92 | 71 | gap |
| YSSB-0650 | 165 | 151.38 | 453.9 | 3.18 | 10.41 | 6 | 0.76 | 5.92 | 64 | gap |
| YSSB-0669 | 170 | 156.38 | 467.2 | 3.18 | 11.18 | 6 | 0.76 | 5.92 | 58 | gap |
| YSSB-0689 | 175 | 154.16 | 480.6 | 3.96 | 8.13 | 6 | 0.81 | 9.53 | 116 | gap |
| YSSB-0709 | 180 | 159.16 | 493.9 | 3.96 | 8.64 | 6 | 0.81 | 9.53 | 105 | gap |
| YSSB-0728 | 185 | 164.16 | 507.3 | 3.96 | 9.14 | 6 | 0.81 | 9.53 | 97 | gap |
| YSSB-0748 | 190 | 169.16 | 520.6 | 3.96 | 9.91 | 6 | 0.81 | 9.53 | 88 | gap |
| YSSB-0787 | 200 | 179.16 | 547.3 | 3.96 | 7.11 | 7 | 0.81 | 9.53 | 174 | gap |
| YSSB-0807 | 205 | 184.16 | 560.7 | 3.96 | 7.37 | 7 | 0.81 | 9.53 | 161 | gap |
| YSSB-0827 | 210 | 189.16 | 578.5 | 3.96 | 7.87 | 7 | 0.81 | 9.53 | 149 | gap |
| YSSB-0847 | 215 | 194.16 | 591.8 | 3.96 | 8.38 | 7 | 0.81 | 9.53 | 138 | gap |
| YSSB-0866 | 220 | 199.16 | 605.2 | 3.96 | 8.64 | 7 | 0.81 | 9.53 | 128 | gap |
| YSSB-0886 | 225 | 204.16 | 618.5 | 3.96 | 7.11 | 8 | 0.81 | 9.53 | 203 | gap |
| YSSB-0906 | 230 | 209.16 | 631.9 | 3.96 | 6.1 | 9 | 0.81 | 9.53 | 303 | gap |
| YSSB-0925 | 235 | 214.16 | 645.2 | 3.96 | 6.35 | 9 | 0.81 | 9.53 | 283 | gap |
| YSSB-0945 | 240 | 219.16 | 658.6 | 3.96 | 6.35 | 9 | 0.81 | 9.53 | 265 | gap |
| YSSB-0984 | 250 | 229.16 | 685.3 | 3.96 | 6.86 | 9 | 0.81 | 9.53 | 232 | gap |
| YSSB-1024 | 260 | 239.16 | 712 | 3.96 | 7.37 | 9 | 0.81 | 9.53 | 205 | gap |
| YSSB-1043 | 265 | 244.16 | 725.3 | 3.96 | 7.62 | 9 | 0.81 | 9.53 | 193 | gap |
| YSSB-1063 | 270 | 249.16 | 743.1 | 3.96 | 8.13 | 9 | 0.81 | 9.53 | 182 | gap |
| YSSB-1102 | 280 | 259.16 | 769.8 | 3.96 | 8.64 | 9 | 0.81 | 9.53 | 162 | gap |
| YSSB-1142 | 290 | 269.16 | 796.5 | 3.96 | 9.4 | 9 | 0.81 | 9.53 | 144 | gap |
| YSSB-1181 | 300 | 279.16 | 823.2 | 3.96 | 10.41 | 9 | 0.81 | 9.53 | 129 | gap |
| YSSB-1221 | 310 | 289.16 | 849.9 | 3.96 | 7.11 | 9 | 1.07 | 9.53 | 264 | gap |
| YSSB-1260 | 320 | 299.16 | 876.6 | 3.96 | 7.62 | 9 | 1.07 | 9.53 | 239 | gap |
| YSSB-1339 | 340 | 319.16 | 934.5 | 3.96 | 8.64 | 9 | 1.07 | 9.53 | 198 | gap |
| YSSB-1378 | 350 | 329.16 | 961.1 | 3.96 | 9.4 | 9 | 1.07 | 9.53 | 180 | gap |
| YSSB-1417 | 360 | 339.16 | 987.9 | 3.96 | 7.62 | 10 | 1.07 | 9.53 | 271 | gap |
| YSSB-1457 | 370 | 349.16 | 1014.6 | 3.96 | 8.13 | 10 | 1.07 | 9.53 | 249 | gap |
| YSSB-1496 | 380 | 359.16 | 1041.3 | 3.96 | 8.64 | 10 | 1.07 | 9.53 | 229 | gap |
| YSSB-1535 | 390 | 369.16 | 1072.4 | 3.96 | 9.14 | 10 | 1.07 | 9.53 | 211 | gap |
| YSSB-1575 | 400 | 379.16 | 1099.1 | 3.96 | 9.65 | 10 | 1.07 | 9.53 | 196 | gap |
| YSSB-1614 | 410 | 382.82 | 1125.8 | 3.96 | 8.38 | 10 | 1.07 | 12.7 | 251 | gap |
| YSSB-1654 | 420 | 392.82 | 1152.5 | 3.96 | 8.89 | 10 | 1.07 | 12.7 | 233 | gap |
| YSSB-1693 | 430 | 402.82 | 1179.2 | 3.96 | 7.62 | 11 | 1.07 | 12.7 | 317 | gap |
| YSSB-1732 | 440 | 412.82 | 1205.9 | 3.96 | 8.13 | 11 | 1.07 | 12.7 | 295 | gap |
| YSSB-1811 | 460 | 432.82 | 1263.7 | 3.96 | 8.89 | 11 | 1.07 | 12.7 | 256 | gap |
| YSSB-1890 | 480 | 452.82 | 1317.1 | 3.96 | 8.13 | 12 | 1.07 | 12.7 | 318 | gap |
| YSSB-1969 | 500 | 472.82 | 1370.5 | 3.96 | 8.89 | 12 | 1.07 | 12.7 | 280 | gap |
| YSSB-2126 | 540 | 512.82 | 1481.8 | 3.96 | 8.89 | 13 | 1.07 | 12.7 | 303 | gap |
| YSSB-2284 | 580 | 552.82 | 1593 | 3.96 | 8.89 | 14 | 1.07 | 12.7 | 327 | gap |
| Weight | 0.0100 |
|---|---|
| Material | 0 |
| Standard Number | No |
| Second Standard | No |
| Drive | 0 |
| Head | 0 |
| American Generic Brand Term | No |
| Diameter | 0 |
| Length | No |